Electrode ya aluminiyumu na aluminiyumuAWS E4043
Ibisobanuro: AWS E4043 ni electrode ya aluminiyumu-silicone ifite irangi rishingiye ku munyu. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse). Gusudira byihuse ku gipimo cy'umuvuduko mugufi. Icyuma cyashyizwemo gifite imbaraga zimwe na zimwe za mekanike kandi kirwanya gucikagurika neza.
Ikoreshwa: . Ikoreshwa mu gusudira plaque ya aluminiyumu, gusuka aluminiyumu na silikoni, aloyi ya aluminiyumu rusange, aluminiyumu ikoze mu byuma na duralumini. Ariko ntikwiriye gusudira aloyi za aluminiyumu na manyeziyumu.
Imiterere ya shimi y'icyuma gisukwa (%):
| Si | Fe | Cu | Mn | Ti | Zn | Al | Mg | Ibindi |
| 4.5 ~ 6.0 | ≤0.8 | ≤0.30 | ≤0.05 | ≤0.20 | ≤0.10 | Komeza | ≤0.05 | ≤0.15 |
Ikoreshwa ry'amashanyarazi risabwa:
| Umwanya w'inkoni (mm) | 3.2 | 4.0 | 5.0 |
| Umuyoboro wo gusudira (A) | 80 ~ 100 | 110 ~ 150 | 150 ~ 200 |
Itangazo:
1. Electrode yoroshye cyane kwangizwa n'ubushuhe, bityo igomba kubikwa mu kintu cyumye gifunguye umwuka kugira ngo idashira bitewe n'ubushuhe; electrode igomba gutekwa ku bushyuhe bwa dogere selisiyusi 150 mu gihe cy'isaha 1 kugeza kuri 2 mbere yo gusudira;
2. Amasahani yo gusudira agomba gukoreshwa mbere yo gusudira, kandi gusudira bigomba gukorwa nyuma yo gushyushya kugeza kuri 200 ~ 300°C hakurikijwe ubunini bw'insinga; inkoni yo gusudira igomba kuba igororotse ku buso bw'insinga, umurambararo ugomba kuba mugufi uko bishoboka kose, kandi gusimbuza inkoni zo gusudira bigomba gukorwa vuba;
3. Ifu yo gusudira igomba gusukurwa amavuta n'imyanda mbere yo gusudira, kandi ifu ikwiye gukurwaho witonze nyuma yo gusudira, hanyuma ikanyuzwa n'umwuka cyangwa amazi ashyushye.
Igihe cyo kohereza: Kamena-05-2023