Amakuru
-
Uruhare rwa Electrode zo Gusudira za Nickel Alloy Stick
Ama-electrode yo gusudira ya Nickel Alloy Stick agenewe ibidukikije bikomeye, afite ubudahangarwa bwiza bwo kwangirika no kudashyuha cyane, kandi akwiriye ibidukikije birimo imiti, ingufu n'ikirere. Ubushobozi bwayo bwo gusudira ibyuma bitandukanye hamwe n'imiterere yayo ihamye y'umurambararo bishobora kugera ku rwego rwo hejuru...Soma byinshi -
Ibyiza bya E71T-8-H8 mu gusudira ibyuma bya karuboni
E71T-8-H8 Icupa rya Karuboni ryikingira ni ibikoresho byo gusudira bifite imikorere myiza cyane byagenewe gusudira ibyuma bya karuboni n'ibyuma bifite aloyi nke. Ntibikenera umwuka wo gukingira inyuma kandi birakwiriye cyane mu bikorwa byo hanze no mu bidukikije bikomeye. Bifite ubushyuhe buke -40℃ ...Soma byinshi -
Imiterere n'ikoreshwa ry'insinga zo gusudira
Insinga zo gusudira ni ibikoresho byo gusudira byiza cyane byagenewe gusudira bihagaze, gusudira imiyoboro ihamye n'indi myanya igoye, byujuje ibisabwa na ASME 5G/6G. Bifite ubushobozi bwo gutuza neza no kudatera imirasire myinshi, bishimangira ubwiza bw'ingufu zo gusudira ku mpande zose, kandi ni...Soma byinshi -
Ku bijyanye n'ingaruka n'imikorere y'ibicuruzwa bya Electrode
Ibikoresho bya electrode ni ibice by'ingenzi by'imikorere myiza ya electrochemical n'ibisubizo by'ingufu, kandi bikoreshwa cyane mu kubika ingufu (nk'amabateri, supercapacitors), ibikoresho by'ubuvuzi (ECG / EEG monitoring) no kugenzura ibidukikije (gusesengura ubuziranenge bw'amazi, gusuzuma umwanda). Ni...Soma byinshi -
Ku bijyanye n'imikorere ya E310-15 Welding Rod
E310-15 Welding Rod yagenewe gusudira ubushyuhe bwinshi n'ingese, kandi ikwiriye guhuza icyuma kitagira umugese cya austenitic n'ibyuma bitandukanye (nk'icyuma kitagira umugese na karuboni). Ifite chromium nyinshi na nikeli itanga ubudahangarwa bwiza bwo gutwika, ubushyuhe bwinshi ...Soma byinshi -
Electrode yo gusudira ya Carbon Steel ifite imikorere myiza yo gusudira ahantu hose
Electrode yo gusudira ya J421 (AWS E6013) ifite potassium rutile coating kugira ngo ikore neza kandi idahindagurika kandi idafite amacandwe menshi. Igishushanyo mbonera cy’iyi electrode gishyigikira gusudira ahantu hose hakoreshejwe ingufu za AC na DC, bigatuma iba nziza cyane mu gukora no gusana. J4...Soma byinshi -
AWS E2209-16 Icyuma gishyushya gifite ubwiza bwo hejuru cya Duplex Stainless Steel Rod
AF2209-16 (AWS E2209-16) ni electrode y'icyuma kitagira umugese ifite kalisiyumu-titanium, irimo azote, ifite karubone nkeya cyane. AWS E2209-16 Stainless Steel Welding Rod yagenewe gukoreshwa mu gusudira ifite imikorere myiza kugira ngo ifashe ingingo zikomeye kandi zirwanya ingese mu bidukikije bikomeye. ...Soma byinshi -
Electrode yo gusudira ibyuma bya karuboni yongera imikorere myiza mu nganda
Electrode yo Gusudira Ibyuma bya Karuboni (501Fe18) ni electrode ikoze neza cyane ya titanium alloy electrode yagenewe gushyiramo vuba. Ikwiriye gusudira mu buryo butambitse/butambitse kandi ishobora gukora umurambararo woroshye hamwe no gusukura gake cyane nyuma yo gusudira. Electrode ya AWS A5.1 E7024 Carbon Steel Weld...Soma byinshi -
Insinga zo gusudira z'umuringa za AWS A5.7 ERCuSn-C zifite ubwiza bwo hejuru
Insinga zo gusudira za AWS A5.7 ERCuSn-C Copper Alloy zagenewe guhuza umuringa n'umuringa-tin. Ubudahangarwa bwiza bwo gutemba no kwangirika butuma ziramba, bigatuma ziba amahitamo meza yo gukoresha mu modoka, mu mazi no mu nganda. Insinga zo gusudira za AWS A5.7 ERCuSn-C Copper Alloy zirahebuje...Soma byinshi -
Insinga zo gusudira za ENiFe-Cl Nickel Alloy Mig zikora neza cyane
Insinga zo gusudira za ENiFe-Cl Nickel Alloy Mig zifite ubushobozi bwiza bwo gusana icyuma gikozwe mu cyuma gishongeshejwe n'icyuma gikozwe mu cyuma gishongeshejwe. Imiterere yayo idafite imiyoboro myinshi ituma icyuma gihagarara neza, ikaba nziza cyane ku modoka, inganda n'imashini ziremereye. Insinga zo gusudira za ENiFe-Cl Nickel Alloy Mig zagenewe gukemura ikibazo...Soma byinshi -
E316-16 Electrodes: Gusudira mu byuma bitagira icyuma bikoreshwa mu bidukikije bikomeye
Electrode za AWS E316-16 zikoresha electrode ya titanium calcium, electrode ya Cr18Ni12Mo2 alloy ifite karubone nkeya, ikwiriye gusudira icyuma kitagira umugese cya 316/316L. Electrode za AWS E316-16 zifite umurambararo uhamye kandi zigabanya imvura ya karubone, kandi zikora neza mu gukoresha imiti, amazi yo mu mazi no mu bushyuhe bwinshi. ...Soma byinshi -
Insinga ikomeye ya AWS A5.23 ECM4 ifite imbaraga nyinshi
Insinga ikomeye ya AWS A5.23 ECM4 yo mu mazi ni electrode ifite alloy nkeya ikoreshwa mu gusudira ifite imbaraga nyinshi. Yujuje ibipimo bya AWS A5.23 M4, ituma imbaraga zo gukurura zirenga 110 ksi, igakomeza gutuza neza no gusudira. Insinga ikomeye ya AWS A5.23 ECM4 yo mu mazi ni ...Soma byinshi