Umutwe: W107 Intangiriro: Inkoni yo gusudira y'icyuma gishyuha cyane

Electrode yo gusudira (3)Mu gusudira ibyuma mu bushyuhe buke, guhitamo electrode ni ingenzi cyane. Aha nihoW107 (AWS E7015-C2L)Ikoreshwa nk'igisubizo cy'ingenzi cyo gusudira ibyuma mu bushyuhe buke. Iyi electrode ifite irangi rya hydrogen sodium nkeya, ikora neza mu bushyuhe buke, ikaba ari yo ihitamo rya mbere mu gusudira mu bidukikije bikomeye.

Imwe mu miterere y'ingenzi ya W107 ni ubushobozi bwayo bwo kugumana ubukana bwiza bw'ingufu ku bushyuhe buri hasi nka -100°C. Ibi bituma iba nziza cyane mu gusudira inyubako z'ibyuma zihura n'ubukonje bukabije, nko mu gihe cyo kubaka ibigega by'amazi, imiyoboro n'ibindi bikorwa remezo mu bihe bikonje. Ubushobozi bw'iyi electrode bwo gukora imashini zisudira zifite ubukana bwiza bw'ingufu ku bushyuhe buke butuma imiterere y'ibikoresho byasudira ikomera kandi ihamye, bigatuma abasudira n'abakora ibintu baruhuka mu mutima.

Uretse kuba ifite imikorere itangaje mu bushyuhe buke, W107 itanga ubushobozi bwo gusudira mu myanya yose, iha abasudira ubushobozi bworoshye bwo kuyikoresha no kuyikoresha. Byaba ari ugusudira mu buryo butambitse, buhagaze cyangwa hejuru y’imashini, W107 itanga ibisubizo bihamye kandi byizewe, bigatuma iba ingirakamaro mu bintu bitandukanye byo gusudira.

Byongeye kandi, W107 yagenewe gukoreshwa na DCEP (Direct Current Electrode Positive Pole), irushaho kunoza imikorere yayo yo gusudira no gukora neza. Ibi byemeza ko electrode ikora neza, itanga ubushude bwiza kandi bunoze kandi butanga umusaruro mwiza. Uruvange rw'ubushobozi bwo gutwikira, ubushobozi bwo gusudira bukoreshwa mu gusimbuza no gushyiramo ibikoresho mu buryo bwa DCEP bituma W107 iba amahitamo meza ku basudira bashaka electrode yizewe kandi ikora neza ijyanye n'ibyo bakeneye mu gusudira ibyuma mu gihe gito.

Muri make, W107 (AWS E7015-C2L) ni yo nkoni yo gusudira icyuma ifite ubushyuhe buke kandi ikora neza cyane, yizewe kandi ikora neza. Ubushobozi bwayo bwo gukomeza gukomera kugeza kuri -100°C, hamwe n'ubushobozi bwayo bwo gusudira no guhuza na DCEP, bituma iba ingirakamaro ku basudira bakorera mu bidukikije bigoye. Hamwe na W107, abasudira bashobora gusudira icyuma gifite ubushyuhe buke bafite icyizere bazi ko bafite electrode nziza ijyanye n'ibyo bakenera mu gusudira.