Insinga zo gusudira zo guhuza ibice bya Martensitic Stainless Steel

Insinga zo gusudirani ingenzi cyane mu bikorwa bitandukanye byo gukora no gusana, ikaba ari ibikoresho byuzuza bikora aho gusonera. ER410NiMo yihariye igaragaza ubwoko bwihariye bw'insinga zikomeye zo gusudira zagenewe gukoreshwa mu buryo bugoye. Nk'insinga y'icyuma kitagira umugese ya martensitic, yakozwe kugira ngo ikore udusonera dukomeye kandi duramba duhuye n'imikorere y'ibikoresho by'ibanze, bigatuma iba ingenzi mu gukora no kubungabunga inganda.

 

Imiterere y'iyi nsinga yo gusudira igenzurwa neza, irimo 11.0-12.5% ​​ya Chromium, 4.0-5.0% ya Nikeli, na 0.40-0.70% ya Molybdenum. Iyi mvange yihariye y'aloyi yakozwe kugira ngo iteze imbere imiterere myiza ya mekanike n'ubuziranenge bw'imiterere y'icyuma cyo gusudira nyuma yo gusudira ndetse n'uburyo ubwo aribwo bwose bwo gusudira nyuma yo gusudira bushyuha. Ingano y'ibi bintu ituma isudira ivamo igira imiterere myiza ya martensitic, ikaba ari ingenzi ku miterere ikenewe mu bikorwa byayo.

 

IbiInsinga zo gusudiraYagenewe by'umwihariko guhuza icyuma cya ASTM CA6NM gikozwe mu byuma bicukurwamo, ibyuma 410/410S/405 bita ibyuma bitagira umugese, n'ibindi bisa nabyo bya 13% bya Chromium – 4% bya Nickel. Ihuye n'ibi bikoresho bituma iba amahitamo meza mu bikorwa by'ingenzi aho ubuziranenge bw'ubucukuzi budakwiye kuganirwaho. Uburyo iyi nsinga yo gusudira ikora butuma icyuma cyo gusudira gishobora kugira uburimbane bwiza mu gukomera, gukomera, no kurwanya ingese, bigahura neza n'iby'ibyuma bikurura.

 

Ubusanzwe iyi nsinga yo gusudira ikoreshwa mu nganda zikora neza cyane. Ikoreshwa cyane mu gukora no gusana ibikoresho bikoresha umuvuduko w’amashanyarazi hakurikijwe amabwiriza y’imiyoboro y’amashanyarazi, ibyuma bya turbine, valves, na sisitemu z’imiyoboro y’amashanyarazi. Yagenewe ibice by’imiterere bisaba uruvange rwo kwirinda ingese no kudashira, bigaragaza imikorere myiza y’iyi nsinga yihariye yo gusudira.

 

ER410NiMo solid Wire ni ikoranabuhanga rigezwehoInsinga zo gusudiraibyo bitanga ibisubizo byizewe kandi bihoraho mu guhuza ibyuma bitagira umugese bya martensitic. Imiterere yabyo yagenzuwe neza hamwe n'uburyo bwo kubikoresha bugamije gutuma biba ibikoresho by'ingenzi mu kurinda igihe kirekire no mu mutekano w'ibice by'ingenzi. Gukoresha iyi nsinga ikwiye yo gusudira ni ingenzi mu kugera ku gusudira byujuje ibisabwa mu nganda kugira ngo bikore neza kandi birambe mu bikorwa bigoye mu gihe hakorerwa serivisi nyinshi.

Insinga zo gusudira