Inkoni ikomeye ya Premium D132 (B-83) itanga uburinzi burambye ku buso

D132 (B-83)Inkoni ikomeyeIgaragara nk'igikoresho cyihariye cyo gusudira gifite hydrogen nke cyakorewe mu bikorwa bikomeye byo gusudira. Iyi arc welding stick irahebuje mu gusubiza ibice byashaje byangiritse mu buryo buciriritse no mu mbaraga zikomeye zo gukanda. Yagizwe inkoni yo gusudira hejuru ndetse n'igisubizo cyo kongera kubaka, itanga arcs zihamye kandi zidapfa gushwanyagurika mu gihe igabanya ibyago byo kwangirika biterwa na hydrogen. Uburyo bwayo butuma ishyirwa mu buryo bworoshye kandi isa neza, bigatuma irushaho kuba nziza mu gusana imashini z'inganda, ibikoresho by'ubuhinzi, n'ibice by'imodoka bisaba gusana no gukomera ku buso.

 

Ibisobanuro bya tekiniki bigaragaza inkoni'ubushobozi budasanzwe. Icyuma gikozwe mu cyuma gifite imbaraga nyinshi zo gukanda kandi gikomeza gukora neza cyane–yemerera ibikorwa byo gusudira nyuma yo gusimbuza nko guhindukira, gusya, no gupanga nta kwangiza ubuziranenge. Iyi miterere ni ingenzi cyane ku bice by'ubuhanga bisaba kwihanganira cyane nyuma yo gusimbuka. Ishyirwa mu byiciro nk'amashanyarazi make ya hydrogène, igabanya cyane ubwiyongere bw'imyenge n'ubukonje bwo kwangirika, cyane cyane mu bice binini cyangwa mu ngingo zifatana cyane. Sisitemu yo gusimbuka neza itanga uburyo bwo gutandukanya imyenge kandi ikagabanya imiyoboro, yongera imikorere myiza.

 

Ku bijyanye n'ibikoresho bisaba ubushobozi bwo kudasaza neza,Inkoni ikomeyeitanga imikorere myiza cyane. Ibigize aloyi birema urwego rukomeye kandi rukora neza, rurwanya kwangirika mu bintu nko mu gutunganya ibikoresho byinshi, mu gukurura ubutaka, cyangwa mu nganda. Bitandukanye n'ibindi bikoresho byoroshye, D132 (B-83)'Ibice byayo bikuramo ingufu z’ingaruka ariko bigakomeza gukomera ku buso, bikongera igihe cyo gukora cyane. Ikwiriye cyane cyane mu kongera kubaka imiyoboro, imigozi, ibice bisya, n’ibyuma by’inganda bihura n’ibibazo byo gukururana no gukandagirana bihoraho.

 

Ibisubizo byiza bisaba gukurikiza ibipimo byo gusudira: Shyushya ibice kugeza kuri 250-300°C (482-572)°F) hashingiwe ku bunini, komeza ubushyuhe bwo hagati y'aho unyura, kandi ukoreshe DC reverse polarity (electrode positive). Bika inkoni mu bikoresho bifunze kuri 250-300°F (121-149)°C) hanyuma wongere uteke iyo uhuye n'ubushuhe buri hejuru ya 50% mu gihe kirenga amasaha 4. Shyira amasaro mu duce duto, tw’imigozi kugira ngo ugenzure uburyo bwo gushonga no kongera ubukana. Nyuma yo gusudira, gukonjesha buhoro buhoro munsi y’ubushyuhe ni byiza kugira ngo wirinde ko hydrogen yangirika.

 

D132 (B-83)Inkoni ikomeyeitanga igisubizo cyizewe kandi gishobora gukoreshwa mu kurwanya kwangirika no kugarura ingano. Imiterere yayo ya hydrogène nke, hamwe n'imbaraga nyinshi zo gukanda no kudashira, bituma iyi mashini yo gusudira hejuru iba ingenzi mu kubungabunga no kongera kubaka mu nganda zikomeye. Mu guhitamo iyi electrode, abahanga mu by'imashini baremeza ko ibice byasubijwe bigarura imikorere yabyo mu gihe bimara igihe kirekire mu bihe bigoye.