ECoCr-A (Cobalt 6) Cobalt Electrode yo gusudira idapfa kwangirika kandi idapfa kwangirika

Ibisobanuro bigufi:

A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods ikoreshwa mu gusudira imitwe ya valve, impeta zifunga za pompe y'umuvuduko mwinshi n'ibice bya crusher.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

ECoCr-A (Cobalt 6) Cobalt Electrode yo gusudira idapfa kwangirika kandi idapfa kwangirika

Ubwoko bw'inyongera: A5.13, Electrode zo hejuru zikomeye n'inkoni zo gusudira, A5.13
ECoCr-A Cobalt Alloy 6 ni yo ikoreshwa cyane mu mabuye akozwe muri cobalt adashira kandi ifite imikorere myiza ku buryo bwose. Ifatwa nk'icyitegererezo cy'inganda mu bikorwa rusange byo kwirinda kwangirika, ifite ubudahangarwa bwiza ku buryo butandukanye bwo kwangirika kwa mekanike na shimi mu bushyuhe bwinshi, kandi igumana ubukana bukwiye kugeza kuri dogere selisiyusi 500 (930⁰F). Inafite ubudahangarwa bwiza ku ngaruka no kwangirika kw'ibice. Cobalt Alloy 6 ikwiriye cyane mu buryo butandukanye bwo gukomera kandi ishobora guhindurwa hakoreshejwe ibikoresho bya karubide.

Ibisanzwe bikoreshwa: ibyuma byo gukata; vali z'amazi zitemba; vis zo gusohora; ibyuma bizunguruka; ubushyuhe bwinshi; ubuso butwara vali

Isomo rya AWS: ECoCr-A Icyemezo: AWS A5.13/A5.13M: 2010
Aloyi: ECoCr-A ASME SFA A5.13

 

Aho gusudira:
F, V, OH, H
Ubu:
*NS

 

Ingufu zo Gukurura, kpsi: *NS
Imbaraga z'umusaruro, kpsi: *NS
Uburebure %: *NS

*NS Ntiyagaragajwe

Ubuhanga busanzwe bw'insinga nk'uko bivugwa na AWS A5.13 (agaciro kamwe ni ntarengwa)

C Mn Si Cr Ni Mo Fe W Co Ibindi
0.7-1.4 2.0 2.0 25-32 3.0 1.0 5.0 3.0-6.0 Rem 1.0