AWS Icyiciro E308HT1-1 / T1-4 Flux Core Wire Umuyoboro Utagira ibyuma Flux-cored Welding Wire

Ibisobanuro bigufi:

AWS E308HT1-1 / T1-4 Flux Core Wire Porogaramu & ikoresha: Ibikoresho byuma.Metallurgie.Imashini.Ubwubatsi.Ubwubatsi bw'ubwato.Ibikomoka kuri peteroli.Uruganda rukora imiti.Urwego rw'amashanyarazi.Inganda za gaz.


Ibicuruzwa birambuye

Ibicuruzwa

AWS Icyiciro E308HT1-1 / T1-4Flux Core WireIbisobanuro

Ibyiciro AWS A5.22, E308HT1-1 / T1-4
Ifishi GusudiraFlux Core Wire
Ubwoko bwo gusudira Gazi Yakingiwe
Ibipimo .045 ”, 1/16”
Gukingira gaze 100% CO2, 75-80% Ar / kuringaniza CO2, 35-50 cfh
Imyanya yo gusudira Imyanya yose
AWS E308HT1-1 / T1-4 Flux Core Wire Porogaramu & ikoresha Ibikoresho byuma
Metallurgie
Imashini
Ubwubatsi
Ubwubatsi bw'ubwato
Ibikomoka kuri peteroli
Uruganda rukora imiti
Urwego rw'amashanyarazi
Inganda za gaz

AWS Icyiciro E308HT1-1 / T1-4 Flux Core Wire Imiti

C Cr Ni Mo Mn Si P S Cu
0.04 18.0-21.0 9.0-11.0 0.75 0.5-2.5 1.0 0.04 0.03 0.75

AWS Icyiciro E308HT1-1 / T1-4 Flux Core Cyuma Cyimashini

Imbaraga za Tensile, kpsi: 75 min
Imbaraga Zitanga, kpsi: NS
Kurambura%: 30 min

AWS Icyiciro E308HT1-1 / T1-4 Flux Core Wire Parameter

Diameter Inzira Volt Amps Gukingira gaze
in (mm)
.035 (.9) GMAW 26-27 150-165 100% CO2
.045 (1.14) GMAW 26-28 160-200 100% CO2
.063 (1.6) GMAW 27-28 215-250 100% CO2

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twagize uruhare mu gukora electrode yo gusudira,gusudira, no gusudira ibikoreshwa mu myaka irenga 20.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.


  • Mbere:
  • Ibikurikira: