Insinga ya AWS A5.22 E312T-1 ifite icyuma kidafunze gifunganye

Ibisobanuro bigufi:

E312T-1 ni insinga y'icyuma kitagira umugese yo mu bwoko bwa AISI 312 ifite imiterere myiza cyane mu gukora.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Insinga ya AWS A5.22 E312T-1 FLUX-CORED

Ibikoresho bya shimi

Fe C Cr Ni Mo Mn Si P S N Cu
Kuringaniza 0.15 28.0-32.0 8.0-10.5 0.5 0.5-2.5 1.0 0.04 0.03 — 0.5

Agaciro kamwe ni ntarengwa keretse iyo byavuzwe ukundi.

Ibisobanuro n'Ikoreshwa
E312T-1 ni insinga ya AISI 312 ifite icyuma kidashonga ifite imiterere myiza cyane. Ikora imiyoboro ikomeye kandi ikomeye ifite imbaraga zo gukurura kurusha ibyuma bya austenitic. Imiyoboro ya solder ihuye n'imiterere n'imiterere ya mekanike ya AISI 312 base metal. Imiyoboro ya solder ni hafi 23 Rockwell C uko ikoreshwa. Imashini zigomba gukorwa buhoro buhoro kuko imiyoboro ya solder irwanya ubushyuhe, ingese no kwangirika. Imiterere yihariye ya metallurgike ni iya ferrite ihagaze muri austenite matrix. Ibi bituma imiyoboro idacika cyane.
Ikoreshwa mu gusudira ibyuma by'ibanze bifite isesengura risa kimwe n'ibyuma bitandukanye. Inweld E312T-1 ikora neza ku byuma birwanya kwangirika, ibyuma bya manganese, ibyuma bikomera, ibyuma bishyuha, icyuma gikingira, icyuma gikingira, ibyuma bitanga umusaruro mwinshi no guhuza ibyuma bishyuha cyane na karubone n'ibyuma bidafite aloyi nyinshi. Ni amahitamo meza cyane nk'urwego rwo hejuru (buffer layer) ku bintu bikomeye.
Imiterere isanzwe y'icyuma gikoreshwa mu gusudira
Ingufu zo Gukurura za AWS Spec: 95.000 psi Ingufu zo Gukuramo: 75.000 psi
Uburebure: 35%

Ibipimo byasabwe
FCAW (DCEP – Electrode +) 100% CO2 cyangwa 75% – 95% Ar / Ingano ya CO2

 

Umurambararo w'insinga Umuvuduko w'amashanyarazi Amperage
0.045” 25-30 130-180
1/16” 24-29 160-250

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora electrodes zo gusudira,inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.