Gusudira mu byuma bitagira umwandaElectrode
AF2209-15
GB/T E2209-15
AWS A5.4 E2209-15
Ibisobanuro: AF2209-15 ni electrode y'icyuma gikozwe mu cyuma gikozwe mu buryo bwa duplex ifite azote nkeya cyane ya karuboni ifite hydrogen nkeya. Koresha DCEP (electrode ifite amashanyarazi ahamye). Imikorere yayo ni myiza cyane. Kubera ko irimo molybdenum na azote, kandi carboni ikaba nkeya cyane, icyuma cyashyizwemo gifite ubushobozi bwo kurwanya imvune no kurwanya stress, cyane cyane stress corruption.
Ikoreshwa: Ikoreshwa cyane cyane mu gusudira ubwoko bumwe bw'ibikoresho by'icyuma kitagira umukungugu bifite karubone nkeya cyane mu nganda za peteroli n'iz'amazi. Nk'ubusudizi bw'icyuma kitagira umukungugu gifite 022Cr22Ni5Mo3N.
Imiterere ya shimi y'icyuma gisukwa (%):
| C | Mn | Si | Cr | Ni | Mo | N | Cu | S | P |
| ≤0.04 | 0.5 ~ 2.0 | ≤0.90 | 21.5 ~ 23.5 | 8.5 ~ 10.5 | 2.5 ~ 3.5 | 0.08 ~ 0.20 | ≤0.75 | ≤0.030 | ≤0.040 |
Imiterere ya tekiniki y'icyuma gisudira:
| Ikintu cyo kugerageza | Imbaraga zo gukurura Mpa | Kurekura % |
| Yemejwe | ≥690 | ≥20 |
Ikoreshwa ry'amashanyarazi risabwa:
| Umwanya w'inkoni (cyangwa semm) | 2.5 | 3.2 | 4.0 | 5.0 |
| Umuyoboro wo gusudira (cyangwa seA) | 50 ~70 | 80 ~ 110 | 130 ~ 150 | 160 ~ 200 |
Itangazo:
1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 250°C mbere yo gusudira;
2. Ni ngombwa gusukura ingese, ibipimo by'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira.
Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, naibikoresho byo gusudiraimyaka irenga 20.
Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.