AWS A5.4 E308L-16 Ibyuma Bitagira Ingufu Bikoresha Electrode zo Gusudira Inkingi zo Gusudira

Ibisobanuro bigufi:

A002 (AWS E308L-16) ni electrode y'icyuma kitagira umugese ya Cr19Ni10 ifite karubone nkeya cyane ifite igipfundikizo cya titanium-calcium


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira mu byuma bitagira umwanda

A002                                                 

GB/T E308L-16

AWS E308L-16

Ibisobanuro: A002 ni electrode y'icyuma kitagira umugese ya Cr19Ni10 ifite karubone nkeya cyane ifite titanium-calcium coating. Ishobora gukoreshwa haba kuri AC na DC ifite imikorere myiza. Ingano ya karubone iri mu cyuma cyashyizwemo ni ≤0.04%, ibyo bikaba bitanga imikorere myiza yo kurwanya ingese hagati y'ibinyabutabire.

Ikoreshwa: Ikoreshwa mu gusudira inyubako z'icyuma kidashonga cyane cya Cr19Ni10, kandi ishobora no gukoreshwa ku nyubako z'icyuma kidashonga cya 06Cr18Ni1Ti kidashonga, ubushyuhe bwacyo buri munsi ya 300°C; ikoreshwa cyane cyane mu gukora insinga z'ubukorikori, ifumbire mvaruganda, peteroli n'ibindi bikoresho.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

9.0 ~ 11.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Kurekura

%

Yemejwe

≥520

≥35

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.0

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 150°C mbere yo gusudira;

2. Koresha amashanyarazi ya DC uko bishoboka kose, kandi umuyoboro w'amashanyarazi ntugomba kuba munini cyane kugira ngo wirinde umutuku w'icyuma cyo gusudira;

3. Ubudahangarwa bw'ubushyuhe n'ingano ya ferrite mu byuma byabitswe bigenwa n'ubwumvikane bubiri bw'ibitangwa n'ibikenewe.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka irenga 20 dukora electrodes zo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.


  • Ibanjirije iyi:
  • Ibikurikira: