AWS A5.4 E309-15 Electrodes z'icyuma kitagira umugese zo gusudira hakoreshejwe intoki, gusudira ibikoresho bikoreshwa mu gusudira

Ibisobanuro bigufi:

A302 (AWS E309-15) ni electrode ya Cr23Ni13 ikoze mu cyuma kitagira umugese ifite umwotsi muke wa hydrogen sodium.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira mu byuma bitagira umwandaElectrode

A307                                      

GB/T E309-15

AWS A5.4 E309-15

Ibisobanuro: A302 ni electrode ya Cr23Ni13 ikoze mu cyuma kitagira umugese ifite sodium nkeya ya hydrogen. Koresha DCEP (electrode ifite umuvuduko ugororotse) kandi ishobora gusukurwa ahantu hose. Icyuma cyashyizwemo gifite ubudahangarwa bwiza bwo kwangirika no kudashonga neza.

Ikoreshwa: Ikoreshwa mu gusudira ubwoko bumwe bw'icyuma kitagira umugese, icyuma gifite ishusho yihariye, icyuma gifite chromium nyinshi, icyuma gifite manganese nyinshi, nibindi.

  

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.15

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

 

Imbaraga zo gukurura

Mpa

Kurekura

%

Yemejwe

≥550

≥25

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.0

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Itangazo:

Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 150°C mbere yo gusudira.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, naibikoresho byo gusudiraimyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo icyuma kitagira umugeseelectrode yo gusudiras, electrode zo gusudira icyuma cya karuboni, electrode zo gusudira zifite alloy nkeya, electrode zo gusudira hejuru, electrode zo gusudira za nikeli na kobalti, insinga zo gusudira zifite icyuma gito n'alloy nkeya, insinga zo gusudira zifite icyuma kidafunze, insinga zikingira gazi, insinga zo gusudira za aluminiyumu, gusudira arc munsi y'amazi. insinga, insinga zo gusudira za nikeli na kobalti, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gukata karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.