AWS E2594-16 Electrode yo gusudira, Inkoni zo gusudira, Ibikoresho byo gusudira

Ibisobanuro bigufi:

AF2594-16 (AWS E2594-16) ni electrode y'icyuma kitagira umugese ifite azote nkeya cyane ifite calcium nyinshi kandi itwikiriwe na titanium-calcium.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira mu byuma bitagira umwandaElectrode

AF2594-16

AWS A5.4 E2594-16

Ibisobanuro: AF2594-16 ni electrode y'icyuma gikozwe mu buryo bwa duplex ifite azote nkeya cyane ifite titanium-calcium coating. Ishobora gukoreshwa haba kuri AC na DC. PRE (agaciro gahwanye n'ubudahangarwa bw'imigozi cyangwa igipimo cy'imigozi) ≥ 40, icyuma gikozwe mu buryo bwa gihanga gifite ubushyuhe bwiza bwo gucika. Bitewe n'uko karubone nkeya n'ingano runaka ya molybdenum na azote, icyuma gikozwe mu buryo bwa gihanga gifite ubudahangarwa bwiza bwo gucika mu migozi no gucika mu migozi.

Ikoreshwa: Ikoreshwa cyane cyane mu gusudira ubwoko bumwe bw'icyuma kitagira umugese cya duplex mu nganda za peteroli, gaze karemano n'ibikomoka kuri peteroli, nka 00Cr25Ni7Mo4N, n'ibindi.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤1.00

24.0 ~ 27.0

8.0 ~ 10.5

3.5 ~ 4.5

0.20 ~ 0.30

≤0.75

≤0.030

≤0.040

 

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Kurekura

%

Yemejwe

≥760

≥15

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(cyangwa semm)

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(cyangwa seA)

50 ~ 80

80 ~ 120

120 ~ 150

150 ~ 200

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 250°C mbere yo gusudira;

2. Ni ngombwa gusukura ingese, ibipimo by'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, naibikoresho byo gusudiraimyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo icyuma kitagira umugeseelectrode yo gusudiras, electrode zo gusudira icyuma cya karuboni, electrode zo gusudira zifite alloy nkeya, electrode zo gusudira hejuru, electrode zo gusudira za nikeli na kobalti, insinga zo gusudira zifite icyuma gito n'alloy nkeya, insinga zo gusudira zifite icyuma kidafunze, insinga zikingira gazi, insinga zo gusudira za aluminiyumu, gusudira arc munsi y'amazi. insinga, insinga zo gusudira za nikeli na kobalti, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gukata karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 