AWS E309L-15 Inkingi zo gusudira mu byuma bitagira umwanda, Electrode yo gusudira mu byuma bitagira umwanda

Ibisobanuro bigufi:

A067 (AWS E309L-15) ni electrode y'icyuma kitagira umugese ya Cr23Ni13 ifite hydrogen sodium nkeya cyane.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira mu byuma bitagira umwandaElectrode

A067                                         

GB/T E309L-15

AWS E309L-15

Ibisobanuro: A067 ni electrode y'icyuma kitagira umugese yo mu bwoko bwa hydrogène Cr23Ni13 ifite hydrogène nkeya cyane. Ikoresha DCEP (electrode y'amashanyarazi ifatika) kandi ishobora gusudira ahantu hose. Ifite carbon nkeya cyane, bityo ishobora kurwanya ingese iterwa n'imvura ya karuboni idafite ibintu biyitera imbaraga nka niobium na titanium.

Ikoreshwa: Ikoreshwa mu buryo bumwe bw'icyuma kitagira umugese, icyuma gikozwe mu buryo buvanze n'ibice by'icyuma bifite imiterere yihariye mu gukora fibre y'ubukorikori, peteroli n'ibindi bikoresho. Ishobora kandi gukoreshwa mu gushyira hejuru y'ibice by'impinduka ku rukuta rw'imbere rw'imiyoboro y'imbaraga za nucleus no gusudira ibice by'imbere by'umunara.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Kurekura

%

Yemejwe

≥520

≥25

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

50 ~ 70

80 ~ 120

130 ~ 160

160 ~ 200

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 300°C mbere yo gusudira;

2. Ni ngombwa gusukura ingese, ibipimo by'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, naibikoresho byo gusudiraimyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.