Insinga zo gusudira za AWS ER5183 Aluminium Udupira two gusudira twa Aluminium MIG n'Insinga za Tig

Ibisobanuro bigufi:

ER5183 ikwiriye gukoreshwa mu gusudira MIG alloy ya aluminium magnesium, imbaraga zo gukurura zikenewe cyane kandi niba icyuma cy'ibanze ari 5083 cyangwa 5654 imbaraga zo gukurura ziba nyinshi cyane. Ikoreshwa cyane mu gusudira imiterere ya aluminium magnesium alloy y'amato, platforms zo mu mazi, locomotives na velomoteurs, moteri, containers, cryogenic velomoteurs n'ibindi.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

ER5183 ikwiriye gukoreshwa mu gusudira MIG alloy ya aluminium magnesium, kandi niba icyuma cy'ibanze ari 5083 cyangwa 5654, imbaraga zo gusudira zaba nyinshi cyane. Ikoreshwa cyane mu gusudira imiterere ya aluminium magnesium alloy y'amato, platforms zo mu mazi, locomotives na velomoteurs, moteri, containers, cryogenic vessels n'ibindi. Ibyuma byayo bisudira bifite ubushobozi bwo kurwanya ingese y'amazi.

Aho gusudira: F, HF, V

Ubwoko bw'umuriro: DCEP

ITANGAZO:

Gukomeza ipaki y'insinga mu buryo bwiza mbere yo gusudira.

Ubuso bugomba gusukurwa hakoreshejwe ubudozi n'insinga byombi bigomba gusukurwa bikurwamo imyanda yandujwe n'amavuta, irangi rya okiside, ubushuhe n'ibindi.

Kugira ngo ubushyuhe bugaragare neza, ni ngombwa gushyushya icyuma cyo hasi kugeza kuri 100℃-200℃ mbere yo gusudira niba ubunini bwacyo ari 10mm cyangwa irenga.

Ni byiza gushyira agace gato munsi y'agace ko gusudira kugira ngo icyuma cyashongeshejwe gitere neza kugira ngo icyuma cyo gusudira kigere neza.

Hakurikijwe aho gusudira n'ubugari bw'icyuma cyo hasi, hagomba gutoranywa gaze zitandukanye zo kurinda, nka 100%Ar, 75%Ar+25%He, 50%Ar+50%He, nibindi.

Imiterere yo gusudira yavuzwe haruguru ni iyo kwifashisha gusa, kandi ni byiza gukora ibizamini by’uburyo bwo gusudira hakurikijwe umushinga mbere yo kubishyira mu gusudira byemewe.

ER5183 IKIMENYETSO CY'IBICURUZWA BYABITSWE (%):

SI FE CU MN MG CR ZN TI AI BE
Igisanzwe ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Kuringaniza ≤0.0003
Ibisanzwe 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Kuringaniza 0.0001

IMITUNGO Y'ICUMA CYABITSWE (AW):

KOMERE Y'UBUKONJE (MPA) UMUSARURO W'INGUFU (MPA) UBUREBURE A4 (%)
Ibisanzwe 280 150 18

Ingano n'Ingano Isabwa Kuri MIG (DC+):

UMUBARE W'INSHINGANO ZO GUSHUSHIRA (MM) 1.2 1.6 2.0
Umuyoboro wo gusudira (A) 180-300 200-400 240-450
Voltage yo gusudira (V) 18-28 20-20 22-34

INGANO N'AMASHANYARAZI Y'INGENZI KURI TIG (DC¯):

UMUBARE W'INSHINGANO ZO GUSHUSHIRA (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Umuyoboro wo gusudira (A) 150-250 200-320 220-400

 

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka irenga 20 dukora electrodes zo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 

 


  • Ibanjirije iyi:
  • Ibikurikira: