Ama-electrode yo gusudira ya Aluminium ya AWS/ASME A 5.3 E1100

Ibisobanuro bigufi:

Ku bijyanye no gusudira aruminiyumu ivanze n'umuringa, silikoni na manyeziyumu. Nanone ni byiza cyane mu guhuza ubwoko butandukanye bwa aluminiyumu.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode ya aluminiyumu na aluminiyumu

L109

GB/T E1100

AWS A5.3 E1100

Ibisobanuro: L109 ni electrode ya aluminiyumu yonyine ifite irangi rishingiye ku munyu. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse). Gerageza gukoresha arc ngufi kugira ngo usuke.

Ikoreshwa: Ikoreshwa mu gusudira amasahani ya aluminiyumu n'ibikoresho bya aluminiyumu byuzuye.

 

Imiterere ya shimi y'icyuma gisukwa (%):

Si+Fe

Cu

Mn

Zn

Al

Ibindi

≤0.95

0.05 ~ 0.20

≤0.05

≤0.10

≥99.0

≤0.15

 

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Yemejwe

≥80

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(cyangwa semm)

3.2

4.0

5.0

Umuyoboro wo gusudira

(cyangwa seA)

80 ~ 100

110 ~ 150

150 ~ 200

 

Itangazo:

1. Electrode yoroshye cyane kwangizwa n'ubushuhe, bityo igomba kubikwa mu kintu cyumye gifunguye umwuka kugira ngo idashira bitewe n'ubushuhe; electrode igomba gutekwa ku bushyuhe bwa dogere selisiyusi 150 mu gihe cy'isaha 1 kugeza kuri 2 mbere yo gusudira;

2. Amasahani yo gusudira agomba gukoreshwa mbere yo gusudira, kandi gusudira bigomba gukorwa nyuma yo gushyushya kugeza kuri 200 ~ 300°C hakurikijwe ubunini bw'insinga; inkoni yo gusudira igomba kuba igororotse ku buso bw'insinga, umurambararo ugomba kuba mugufi uko bishoboka kose, kandi gusimbuza inkoni zo gusudira bigomba gukorwa vuba;

3. Ifu yo gusudira igomba gusukurwa amavuta n'imyanda mbere yo gusudira, kandi ifu ikwiye gukurwaho witonze nyuma yo gusudira, hanyuma ikanyuzwa n'umwuka cyangwa amazi ashyushye.

 

 

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka irenga 20 dukora electrodes zo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 

EN 573-3: E Al

DIN: 1732: EL-Al

IBIKORESHO N'IMITERERE:

Ku bijyanye no gusudira aruminiyumu ivanze n'umuringa, silikoni na manyeziyumu. Nanone ni byiza cyane mu guhuza ubwoko butandukanye bwa aluminiyumu.

Electrode yo gusudira arc ya aluminiyumu yuzuye hamwe n'icyuma cyihariye cyo kuyizamura. Hari n'izindi ngero za aluminiyumu nka 12%Si, 5%Si na Al Mn, n'ibindi.

Imashini idasanzwe yo kwiterura.

Irangi ry'umweru mwiza kandi rimara igihe kirekire rirusha iry'ibicuruzwa bisanzwe mu gihe cyo kwirinda ubushuhe.

Ishobora gukorwa mu mabara atandukanye yihariye.

Iboneka mu ducupa twa ALUMINUM DUFITE AGACIRO K'UMUNTU ...

Isesengura ry'icyuma cyose cya Welded Metal (Uburemere busanzwe %):

Ibara ryiza: Amabara y'umweru cyangwa ay'umwihariko

Si Cu Fe Ti Mn Zn Be Al
.091 .05 .45 .01 .005 .002 .0002 Umupira w'inyuma.

IMITUNGO ISANZWE YA KENIKI:

Ibyuma bitavanze kandi bidafite imvange Agaciro ntarengwa Kugeza kuri:

Ingufu zo Gukurura: 34.000 psi (250 N/MPa)

Ingufu z'umusaruro: 20.000 psi (150 N/MPa)

Uburebure: 5%

Gusudira n'amabwiriza yo gukoresha ubushyuhe
Ikoreshwa ry'amashanyarazi: DC Isubira inyuma (+)
Ingano (mm) 3/32 (2.5) 1/8 (3.25)
Ingano ntoya y'ampeta 50 70
Ingufu ntarengwa 80 120

Uburyo bwo gusudira: Tangira ukoresheje igice cyo hejuru cy'urugero rwa amperage. Shyira electrode vuba kandi ugende vuba ukomeza kugira icyuho cy'arc hafi cyane.

Ahantu ho gusudira: Hafu, Hatambitse

IBIPIMO BYO GUTANGA IMYENDA:

Ingano (mm) Uburebure (mm) Ibyuma bisukwa/Electrode Electrodes perlb (kg) ya Weldmetal Igihe cyo Gushyiramo iminota/lb (kg) Igenamiterere rya Amperage Igipimo cyo kugarura
3/32 (2.5) 14″ (350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14″ (350) 0.23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14″ (350) 0.33oz (9.6g) 48 (107) 47 (103) 135 90%

IPAKISHO N'INGANO BY'AMASHANYARAZI:

Ingano (mm) 3/32 (2.5) 1/8 (3.25) 5/32 (4.0)
Uburebure (mm) 14″ (350) 14″ (350) 14″ (350)
Electrode / lb 49 33 23
Electrode / kg 108 73 51

  • Ibanjirije iyi: