Insinga yo gusudira ya E2209T1-1/T1-4 Icunga ry'Icyuma Kidafunze

Ibisobanuro bigufi:

Ikozwe neza mu gusudira mu buryo bugororotse, haba mu buryo buhagaze hejuru cyangwa mu buryo buhamye bwo gusudira mu buryo bwa ASME 5G cyangwa 6G (umuyoboro ubusanzwe ufite umurambararo wa mm 150, > urukuta rwa mm 15).
Gutunganya uburyo bwo gusudira ahantu hose


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Icyiciro cya AWS E2209T1-1/T1-4Insinga ya Flux Core

IBIKORESHO
Yakozwe neza mu gusudira mu buryo buhamye, haba mu buryo buhagaze hejuru no mu buryo buhamye, ifite ubushobozi bwo gusudira mu buryo bwa ASME 5G cyangwa 6G (umuyoboro ubusanzwe ufite umurambararo wa mm 150, > urukuta rwa mm 15).
Gutunganya uburyo bwo gusudira ahantu hose
Gukuraho ibishingwe neza cyane

Gazi yo kurinda
80% Argon / 20% CO2
CO2 100%

Ibiranga by'ingenzi
• Koroshya uburyo bwo gusudira ahantu hose
• Ipaki ifunze neza
• Gukuraho neza amacandwe
• Icyemezo kigaragaza imiterere y'ibicuruzwa byatanzwe, inomero ya ferrite, n'imiterere ya charpy impact yapimwe kuri -196°C (-320°F)

Icyiciro cya AWS E2209T1-1/T1-4Insinga ya Flux CoreIbikoresho bya shimi

C Cr Ni Mo Mn Si P S N Cu
.03 22.5 9.7 3.25 0.95 .60 0.03 .015 0.14 0.20
Imiterere ya Mechanical y'Insinga ya Flux Core ya AWS Class E2209T1-1/T1-4 Flux Core
Imbaraga zo Gufata 120.000 psi
Imbaraga z'umusaruro 95,000 psi
Uburebure (%) 26%
Ibipimo by'insinga za AWS Class E2209T1-1/T1-4 Flux Core
Ingano WFS (ipm) Amperage Volti ESO (muri.) Igipimo cyo Gutanga Amafaranga
(ibiro/isaha)
.045” 250 130 22 5/8-3/4” 5.4
300 160 24 5/8-3/4” 6.3
425 200 26 5/8-3/4” 9.2
780 270 32 5/8-3/4” 16.2
1/16” 150 170 23 3/4-1” 5.4
195 215 25 3/4-1” 7.0
240 250 26 3/4-1” 8.6
320 305 27 3/4-1” 11.5

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora electrodes zo gusudira,inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.