E316HT1-1 Insinga y'icyuma kidasesagura ikoreshwa mu gukurura
Ibisobanuro by'igicuruzwa
Ikurikije ibipimo ngenderwaho: GB/T17853 E316T1-1
AWS A5.22 E316HT1-1
Ibiranga n'Imikoreshereze
1. Kubera ko irimo ingano runaka ya karuboni, ikwiriye gusudira ibikoresho by'icyuma kidashyuha cyane;
2. Ifite imikorere myiza yo gusudira nko gupfuka imirasire ihamye, gupfuka imirasire mike, gukuraho imirasire neza, gukwirakwiza insinga ihamye, n'imiterere myiza;
3. Bitewe n'ubwinshi bwa Mo, ubushobozi bwo kurwanya ingese burakomeye;
4. Bikwiriye gusudira 18% Cr-12% Ni-2% Mo mu nganda zikora peteroli, mu cyuma gishyushya, mu mashini zikora imiti n'ibiribwa, mu nganda zikora ifumbire mvaruganda n'izindi nganda.
Ibikubiye mu binyabutabire (wt%)
| Uburemere bw'aloyi% | C | Mn | Kandi | Cr | In | Mo | P | S | Hamwe na |
| GB/T | 0.08 | 0.5-2.5 | 1.0 | 17.0-22.0 | 11.0-14.0 | 2.0-3.0 | 0.040 | 0.030 | 0.50 |
| AWS | 0.04-0.08 | 0.5-2.5 | 1.0 | 17.0-22.0 | 11.0-14.0 | 2.0-3.0 | 0.040 | 0.030 | 0.75 |
| Agaciro k'urugero | 0.50 | 1.45 | 0.50 | 18.05 | 12.00 | 2.35 | 0.020 | 0.005 | 0.05 |
Imyitwarire ya mekanike
| Imyitwarire ya mekanike | MPa ifite imbaraga zo gutanga umusaruro | MPa ifite imbaraga zo gukurura | Uburebure% | Agaciro k'ingaruka J/℃ |
| GB/T | - | 520 | 30 | - |
| AWS | - | 520 | 30 | - |
| Agaciro k'urugero | - | 560 | 35 | - |
Ingano y'ubushyuhe isabwa: (DC+)
| Umurambararo w'insinga zo gusudira (mm) | 1.2 | 1.6 |
| Voltage (V) | 22-36 | 26-38 |
| Umuvuduko w'amashanyarazi (A) | 120-260 | 200-300 |
| Uburebure bwumutse (mm) | 15-20 | 18-25 |
| Urujya n'uruza rwa gaze (l/min) | 15-25 | 15-25 |
Amabwiriza yo Kwirinda Gusudira
1. Koresha umwuka urinda CO2 ufite ubuziranenge bwa ≥99.98% n'umuvuduko wa gazi wa 20-25L/min.
2. Ubushyuhe hagati y'imiyoboro: 16~100 ℃.
3. Mu gusudira, ni ngombwa kurinda umuyaga kugira ngo wirinde ko gazi yo gusudira ikwirakwira. Amavuta, amazi, n'ibindi aho gusudira bigomba gukurwaho.
4. Koresha insinga yo gusudira vuba bishoboka nyuma yo gufungura ipaki. Niba idakoreshejwe, fata ingamba zo kwirinda ubushuhe.
Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora electrodes zo gusudira,inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.
Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.