A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods ikoreshwa mu gusudira imitwe ya valve, impeta zifunga za pompe y'umuvuduko mwinshi n'ibice bya crusher.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

 

AWS Imvugo: AWS A5.13 / AME A5.13 ECoCr-C
IBIKORESHO:

Ubuso bukomeye bw'imitwe ya valve, impeta zifunga za pompe y'umuvuduko mwinshi n'ibice by'ibyuma bisya.
IBISOBANURO:

Electrode itwikiriwe na COBALTARD 1FC ni yo aluminium isanzwe ifite ubukana bwinshi mu itsinda ry’ibyuma bya kobalti bikoreshwa mu kwangirika kw’ubushyuhe bwinshi bifitanye isano no kwangirika. Ibice by’iyi aluminium bifite chromium carbides nyinshi bigira ingaruka ku kwangirika gukomeye. Kongeramo tungsten byongera ubukana bw’ubushyuhe bwinshi no gukomera kwa matrix kugira ngo ifashe neza kole no kwangirika kw’uduce duto. Ifatana neza n’ibyuma byose, harimo n’ibitagira umugese.
IBISOBANURO KU MIKORESHEREZE:

Shyushya kuri dogere selisiyusi 300 no hejuru muri rusange. Koresha uduti twerekana ubushyuhe bwa PHILARC cyangwa icyuma gipima ubushyuhe cya PHILARC kugira ngo umenye niba ubushyuhe bukwiye bugerwaho mbere yo gusudira. Ku bindi bisobanuro reba Imbonerahamwe ya PHILARC Intambwe 4 zoroshye zo gusudira.

Bifasha gushyushya kuri dogere selisiyusi 600 no gukonjesha buhoro nyuma yo gusudira kugira ngo hirindwe ko byacika.

Shyira electrodes kuri 150-200ºC mu gihe cy'iminota 30 - 60 mbere yo kuzikoresha. Koresha ifuru zumisha zigendanwa za PHILARC.

UBUKOMERE BW'IBITSEHO BY'ICUMA BYO GUSUDURA: HRC 50 – 56 (Hv 520- 620)
IMITERERE ISANZWE Y'IBYUMA BYO GUSUDURA (%):

C Si Mn Cr W Co
2.15 0.47 1.03 31.25 12.72 Umupira

INGANO ZIHARI KANDI ZISANZWE (DC +):

Ingano (mm) 3.2 4.0 5.0
Uburebure (mm) 350 350 350
Ingano y'Ubu (Amp) 90 - 120 110 - 150 140 - 180

 

 