Insinga zo gusudira za ER5356 Aluminiyumu zo gusudira Insinga na Electrode

Ibisobanuro bigufi:

ER5356 ni ubwoko rusange bwa aluminiyumu ikoreshwa mu buryo rusange, akenshi itoranywa kubera imbaraga zayo zo gukata cyane.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

ER5356 ni ubwoko bwa aluminiyumu bukoreshwa muri rusange, akenshi butoranywa kubera imbaraga zayo zo gukata. Byongeye kandi, inatanga ubushobozi bwo kurwanya ingese iyo ihuye n'amazi y'umunyu. ER5356 ikwiye kwitabwaho mu gusudira ibyuma 5000 by'uruhererekane rwa aluminiyumu.

Ibisanzwe bikoreshwa: insinga zo gusudira

Isomo rya AWS: ER5356 Icyemezo: AWS A5.10/ A5.10M: 1999
Aloyi: ER5356 AWS/ASME SFA A5.10
Aho gusudira:
F, V, OH, H
Ubu:
DCEP-GMAW
AC-GTAW
Imiterere isanzwe (nk'uko ishongeshejwe)
Uburyo bwo kuyobora amashanyarazi: 29% IACS (-0)/27% IACS (-H18)
Ingufu zo Gukurura, kpsi: 38
Ibara: Umweru
Aho gushonga 1175⁰F Gukomera 1060⁰F Ubucucike Ibiro 0.096/cu.
Ubuhanga busanzwe bw'insinga nk'uko bivugwa muri AWS A5.10 (agaciro kamwe ni ntarengwa)
Si Fe Cu Mn Mg Cr Zn Ti Ibindi AL
0.25 0.40 0.10 0.50-1.0 4.7-5.5 0.05-0.20 0.25 0.05-0.20 0.15 Ibisigaye
Ibipimo bisanzwe byo gusudira
Ingano Inzira Volti Amps GAZI
in (mm)
.030 (.8) GMAW 15-24 60-175 Argon (cfh)
.035 (.9) GMAW 15-27 70-185 Argon (cfh)
3/64” (1.2) GMAW 20-29 125-260 Argon (cfh)
1/16” (1.6) GMAW 24-30 170-300 Argon (cfh)
3/32” (2.4) GMAW 26-31 275-400 Argon (cfh)
Ingano Inzira Volti Amps GAZI
in (mm)
1/16” (1.6) GTAW 15 60-80 Argon (cfh)
3/32” (2.4) GTAW 15 125-160 Argon (cfh)
1/8” (3.2) GTAW 15 190-220 Argon (cfh)
5/32” (4.0) GTAW 15 200-300 Argon (cfh)
3/16” (4.8) GTAW 15-20 330-380 Argon (cfh)

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka irenga 20 dukora electrodes zo gusudira, inkoni zo gusudira, n'ibikoresho byo gusudira.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 

 


  • Ibanjirije iyi:
  • Ibikurikira: