Insinga yo gusudira ifite imiterere ya Flux, Ingano: Insinga ya A 5.22 E308L T1-1 Icunga Indabyo

Ibisobanuro bigufi:

Ku byuma bisudira icyuma gipima karuboni nkeya 18-20% Cr/ 8-12% Ni bifite ubushobozi bwo gusudira neza Kubera ko ferrite ihari, icyuma gisudira gifite ubushobozi buke bwo kwangirika. Imiterere ya mekanike ni myiza cyane iyo isundiwe kandi ifite ubushobozi bwo kurwanya ingese hagati y’ibice binini bitewe n’uko karuboni nkeya.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Flux Cored Insinga zo gusudira, Icyiciro: A 5.22 E308l T1-1

Ibisobanuro by'ibicuruzwa

Ibikoresho by'insinga SS
Ingano kuri buri mubumbe ibiro 15
Gupfunyika Ibiro 15 kuri buri paki
Icyiciro A 5.22 E308L T1-1
Ubwoko bwo gupfunyika Igipfundikizo gipfundikishijwe mu ishashi ya pulasitiki kandi gipfundikishijwe mu gasanduku gakozwe mu ibumba
Ubunini 1.2MM 1.6MM
Ubu 190-300A
Kwagura insinga 20-25mm (ifite uburebure bwa milimetero 10)
Ingano iboneka 2.00mm, 2.4mm
Polarité Insinga ya DC ifite ubuziranenge
Gazi yo kurinda Gazi ya CO2 ifite igipimo cy'amazi kiri hagati ya litiro 15-20 ku munota
Imiterere ya Mechanical yo Gusudira UTS=520N/mm2 Min; Uburebure(%)=35% min
Ubutabire bw'icyuma busudishwa C = 0.035%, Mn = 1,65%, P = 0,02%, Si = 0,50%, S = 0.008%, Ni = 9.50%, Cr = 19.50%

Ibisobanuro by'igicuruzwa
Insinga y'icyuma kitagira umugozi ifite umurambararo uhamye kandi woroshye, hamwe n'uburyo bworoshye bwo gutandukanya slag

Porogaramu:
Ku byuma bisudira icyuma gipima karuboni nkeya 18-20% Cr/ 8-12% Ni bifite ubushobozi bwo gusudira neza Kubera ko ferrite ihari, icyuma gisudira gifite ubushobozi buke bwo kwangirika. Imiterere ya mekanike ni myiza cyane iyo isundiwe kandi ifite ubushobozi bwo kurwanya ingese hagati y’ibice binini bitewe n’uko karuboni nkeya.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora electrodes zo gusudira,inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.