Electrode yo Gusudira ya G202 Icuma Kidafunze, GB/T E410-16 Inkingi zo Gusudira ku Mpando Zose

Ibisobanuro bigufi:

G202 (GB/T E410-16) ni electrode ya Cr13 ikoze mu cyuma kitagira umugese ifite igifuniko cya titanium calcium. Ishobora gukoreshwa mu gusudira ahantu hose hamwe na AC na DC.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira mu byuma bitagira umwandaElectrode

G202                                                     

GB/T E410-16

Ibisobanuro: G202 ni electrode ya Cr13 ikoze mu cyuma kitagira umugese ifite igifuniko cya titaniyumu. Ishobora gukoreshwa mu gusudira ahantu hose hamwe na AC na DC.

Ikoreshwa: Ikoreshwa mu gusudira inyubako z'icyuma kidasagwa cya 06Cr13 na 12Cr13, kandi ishobora no gukoreshwa mu gusudira ubuso budashobora kwangirika cyangwa kwangirika.

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0. 12

≤1.0

≤0.90

11.0 ~ 13.5

≤0.7

≤0.75

≤0.75

≤0.03

≤0.04

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Kurekura

%

Yemejwe

≥450

≥20

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

80 ~ 120

100 ~ 160

150 ~ 200

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 150°C mbere yo gusudira;

2. Imashini yo gusudira igomba gushyuha kugeza kuri 250 ~ 350°C mbere yo gusudira.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 

 


  • Ibanjirije iyi: