GB/T EZNiCu-1 (Z508) Icupa ry'icyuma rikozwe mu cyuma gishongeshejwe Electrode ya Nickel-Copper Alloy (Monel) Core and Graphitized Coating

Ibisobanuro bigufi:

GB/T EZNiCu-1 (Z508) ni electrode ikoreshwa mu gusudira icyuma gikozwe mu cyuma gifite inkingi ya nikeli-umuringa (Monel) hamwe n'igitambaro cya grafiti.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira mu byuma bikozwe mu ibumbaElectrode

Z508                                                     

GB/T EZNiCu-1

Ibisobanuro: Z508 ni electrode yo gusudira icyuma ikozwe mu cyuma gifite ishingiro rya nickel-copper (Monel) hamwe n'igitambaro cya graphize. AC na DC bifite intego ebyiri, arc ihamye, byoroshye kuyikoresha. Uburyo bwo kuyikora no kuyikata ni hafi ya Z308, ariko bitewe n'uko icyuma cyashyizwemo cyagabanutse cyane, ubushobozi bwo kuyicamo buragabanuka. Ingufu z'imigozi zisutswe ni nke, bityo ntizikwiriye gusudira ibice bikomeye.

Imikoreshereze: Ikoreshwa mu gusana imashini zisuka mu cyuma cy'imvi zidasaba imbaraga nyinshi.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Si

Mn

Fe

S

Ni

Cu

Ibindi

0.35 ~ 0.55

≤0.75

≤2.3

3.0 ~ 6.0

≤0.025

60 ~ 70

25 ~ 35

≤1.0

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

90 ~ 110

120 ~ 150

160 ~ 190

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe hafi 150°C mbere yo gusudira;

2. Mu gusudira, ni byiza gukoresha inzira nto, kandi uburebure bwa buri gusudira ntibugomba kurenza mm 50. Hita ukubita isudira ukoresheje inyundo nto kugira ngo ugabanye ubukana bw'aho gusudira kandi wirinde ko hacikamo ibice nyuma yo gusudira.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora electrodes zo gusudira, inkoni zo gusudira, naibikoreshwa mu gusudiras mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 


  • Ibanjirije iyi:
  • Ibikurikira: