Insinga zo gusudira za Nickel Alloy ERNiCrCoMo-1 Nickel Tig Wire Filler Metal

Ibisobanuro bigufi:

Alloy 617 (ERNiCrCoMo-1) ni insinga ifite ubushyuhe bwinshi ikoreshwa mu gusudira alloys za nickel-chromium-cobalt-molybdenum.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Aloyi ya nikeliInsinga zo gusudiraInsinga ya TigERNiCrCoMo-1

 

Amahame
EN ISO 18274 - Ni 6617 - NiCr22Co12Mo9
AWS A5.14 – ER NiCrCoMo-1

 

Ibiranga na Porogaramu

Alloy 617 ni insinga ifite ubushyuhe bwinshi ikoreshwa mu gusudiranikeli-aloyi za chromium-cobalt-molybdenum.

Ni byiza cyane mu gupfuka aho bikenewe ko habaho ifu nk'iyi, nka turbine za gaze n'ibikoresho bya ethylene.

Bikwiriye guhuza aloyi zitandukanye aho imbaraga z'ubushyuhe bwinshi n'ubudahangarwa bwa ogisijeni biba bikenewe kugeza kuri 1150°C.

Ubusanzwe ikoreshwa mu nganda zikora indege n'ingufu, harimo n'inganda zikora peteroli mu bikorwa nka aside nitrique catalyst grids n'ibindi.

Ibikoresho bisanzwe by'ibanze

Inconel alloys 600 na 601, Inconel alloys 800 HT na 802 hamwe n'alloys zakozwe nka HK40, HP na HP45 Modified. Nimero ya UNS N06617, 2.4663, 1.4952, 1.4958, 1.4959, NiCr21Co12Mo, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 21, Alloy 617, N08810, N08811*
* Urutonde rw'ibishushanyo, ntabwo ari urusobe rw'ibintu byose

 

 

Ibikubiye mu binyabutabire %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

0.05

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

0.10

1.00

1.00

0.020

0.015

0.50

0.50

Ni%

Ko%

Al%

Ti%

Cr%

Mo%

44.00

10.00

0.80

umubare ntarengwa

20.00

8.00

umunota

14.00

1.50

0.60

24.00

10.00

 

Imiterere ya mekanike
Imbaraga zo Gufata ≥620 MPa
Imbaraga z'umusaruro -
Kurekura -
Imbaraga z'Ingaruka -

Imiterere ya mekanike ni iyo hafi kandi ishobora gutandukana bitewe n'ubushyuhe, imyuka ikingira, ibipimo byo gusudira n'ibindi bintu.

 

Imyuka yo kurinda

EN ISO 14175 - TIG: I1 (Argon)

 

Imyanya yo gusudira

EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Amakuru yo gupakira

Ingano

Uburebure

Uburemere

mm 1.60

mm 2.40

mm 3.20

mm 1000

mm 1000

mm 1000

Ibiro 5

Ibiro 5

Ibiro 5

 

Inshingano: Nubwo hakozwe ibishoboka byose kugira ngo amakuru ari muri ibyo abe ari ukuri, aya makuru ashobora guhinduka nta nteguza kandi ashobora gufatwa nk'akwiriye gusa nk'ubuyobozi rusange.


  • Ibanjirije iyi:
  • Ibikurikira: