Aloyi ya nikeliInsinga zo gusudiraInsinga ya TigERNiCrMo-10
| Amahame |
| EN ISO 18274 - Ni 6022 - NiCr21Mo13Fe4W3 |
| AWS A5.14 – ER NiCrMo-10 |
Ibiranga na Porogaramu
Aloyi ya nikeli-chromium-molybdenum yagenewe guhuza C22, 625, 825 cyangwa uruvange rw'izi aloyi.
Itanga icyuma gikomeye cyo gusudira kidafite Nb ku byuma bitandukanye bisa mu byuma bitagira icyuma na super austenitic na super duplex.
Itanga ubudahangarwa bwiza bwo kurwanya stress & corruption, corruption and fractured corruption.
Ikoreshwa cyane mu gupfunyika no gupfunyika ibyuma byo hasi.
Ubusanzwe ikoreshwa mu gusudira ibikoresho byangiza cyane mu nganda zitunganya imiti, ahantu hadakoreshwa ingese ndetse no mu nyubako zikomeye zo mu nyanja no mu bikomoka kuri peteroli n'ibindi.
Impamyabumenyi z'ibizamini urashobora kuzisanga kuri interineti @wilkinsonstar247.com
Ibikoresho bisanzwe by'ibanze
Aloi 22, Aloi 625, Aloi 825, Aloi 926*
* Urutonde rw'ibishushanyo, ntabwo ari urusobe rw'ibintu byose
| Ibikubiye mu binyabutabire % | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | Cu% |
| umubare ntarengwa | umubare ntarengwa | 2.00 | umubare ntarengwa | umubare ntarengwa | umubare ntarengwa | umubare ntarengwa |
| 0.010 | 0.50 | 6.00 | 0.020 | 0.010 | 0.08 | 0.50 |
| Ni% | Ko% | Cr% | Mo% | V% | W% | |
| 49.00 | umubare ntarengwa | 20.00 | 12.50 | umubare ntarengwa | 2.50 | |
| umunota | 2.50 | 22.50 | 14.50 | 0.30 | 3.50 | |
| Imiterere ya mekanike | ||
| Imbaraga zo Gufata | ≥690 MPa | |
| Imbaraga z'umusaruro | - | |
| Kurekura | - | |
| Imbaraga z'Ingaruka | - | |
Imiterere ya mekanike ni iyo hafi kandi ishobora gutandukana bitewe n'ubushyuhe, imyuka ikingira, ibipimo byo gusudira n'ibindi bintu.
Imyuka yo kurinda
EN ISO 14175 - TIG: I1 (Argon)
Imyanya yo gusudira
EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG
| Amakuru yo gupakira | |||
| Ingano | Uburebure | Uburemere | |
| mm 1.60 | |||
mm 2.40
3.20 mm1000 mm
mm 1000
1000 mm5 kg
Ibiro 5
Ibiro 5
Inshingano: Nubwo hakozwe ibishoboka byose kugira ngo amakuru ari muri ibyo abe ari ukuri, aya makuru ashobora guhinduka nta nteguza kandi ashobora gufatwa nk'akwiriye gusa nk'ubuyobozi rusange.