Insinga zo gusudira za Nickel Alloy Insinga zo gusudira za ERNiCrMo-3 Mig

Ibisobanuro bigufi:

ERNiCrMo-3 ni insinga ifite nikeli nyinshi yakozwe mu gusudira no gupfuka aloyi zishingiye kuri nikeli nka 625 cyangwa ibindi bisa nayo.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Aloyi ya nikeliInsinga zo gusudiraERNiCrMo-3

 

Amahame

EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb

AWS A5.14 – ER NiCrMo-3

 

Ibiranga na Porogaramu

Hejurunikeliinsinga z’icyuma zakozwe mu gusudira no gupfuka aloyi zishingiye kuri nikeli nka 625 cyangwa ibindi bisa nabyo.

Ishushanyije neza mu buryo bwihariye kugira ngo ibone ibikoresho byo gusudira byiza kandi byiza cyane bifite umushoro mwiza kandi biramba neza.

Icyuma cyo gusudira gifite ubushobozi bwiza cyane bwo gukora mu bushyuhe buri hejuru n'ubukonje.

Ubudahangarwa bwiza ku myobo no kwangirika kw'imitsi.

Ubushyuhe bw'akazi busabwa buri hagati ya cryogenic na 540°C.

Uburyo bwo gushyiramo insinga neza butuma ikoreshwa neza.

Ikoreshwa cyane mu nganda zitunganya imiti, ubwubatsi bwo mu mazi, ibice by'ingufu za kirimbuzi, indege no mu bikoresho byo kugenzura ihumana n'ibindi.

 

Ibikoresho bisanzwe by'ibanze

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926* * Urutonde rw'ibishushanyo, ntabwo ari uruhererekane rwuzuye

 

Ibikubiye mu binyabutabire %

C%

Mn%

Fe%

P%

S%

Si%

Cu%

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Ko%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

umubare ntarengwa

umubare ntarengwa

umubare ntarengwa

20.00

3.15

8.00

Iminota

1.0

0.40

0.40

23.00

4.15

10.00

 

Imiterere ya mekanike

Imbaraga zo Gufata

≥760 MPa

Imbaraga z'umusaruro

≥415 MPa

Kurekura

≥35%

Imbaraga z'Ingaruka

≥100 J

Imiterere ya mekanike ni iyo hafi kandi ishobora gutandukana bitewe n'ubushyuhe, imyuka ikingira, ibipimo byo gusudira n'ibindi bintu.

Imyuka yo kurinda

EN ISO 14175 – I1, I3

Imyanya yo gusudira

EN ISO 6947 - PA, PB, PC, PD, PE, PF

Amakuru yo gupakira

Ingano

Uburemere

Spool

Umubare w'amapaleti

1.00 mm

mm 1.20

Ibiro 15

Ibiro 15

BS300

BS300

72

72