Aloyi ya nikeliInsinga zo gusudiraInsinga ya TigERNiCrMo-3
Ibiranga na Porogaramu
Hejurunikeliinsinga z'ibyuma byakozwe mu gusudira no gupfukanikeliibishushanyo mbonera bishingiye kuri aluminiyumu nka 625 cyangwa ibindi bisa nabyo.
Ishushanyije neza mu buryo bwihariye kugira ngo ibone ibikoresho byo gusudira byiza kandi byiza cyane bifite umushoro mwiza kandi biramba neza.
Icyuma cyo gusudira gifite ubushobozi bwiza cyane bwo gukora mu bushyuhe buri hejuru n'ubukonje.
Ubudahangarwa bwiza ku myobo no kwangirika kw'imitsi.
Ubushyuhe bw'akazi busabwa buri hagati ya cryogenic na 540°C.
Ikoreshwa cyane mu nganda zitunganya imiti, ubwubatsi bwo mu mazi, ibice by'ingufu za kirimbuzi, indege no mu bikoresho byo kugenzura ihumana n'ibindi.
Ibikoresho bisanzwe by'ibanze
Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926*
* Urutonde rw'ibishushanyo, ntabwo ari urusobe rw'ibintu byose
| Amahame |
| EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb |
| AWS A5.14 – ER NiCrMo-3 |
| Ibikubiye mu binyabutabire % | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | Cu% |
| umubare ntarengwa | umubare ntarengwa | umubare ntarengwa | umubare ntarengwa | umubare ntarengwa | umubare ntarengwa | umubare ntarengwa |
| 0.10 | 0.50 | 0.50 | 0.015 | 0.015 | 0.50 | 0.50 |
|
|
|
|
|
|
|
|
| Ni% | Ko% | Al% | Ti% | Cr% | Nb+Ta% | Mo% |
| 60.00 | umubare ntarengwa | umubare ntarengwa | umubare ntarengwa | 20.00 | 3.15 | 8.00 |
| umunota | 1.0 | 0.40 | 0.40 | 23.00 | 4.15 | 10.00 |
| Imiterere ya mekanike | ||
| Imbaraga zo Gufata | ≥760 MPa | |
| Imbaraga z'umusaruro | ≥415 MPa | |
| Kurekura | ≥35% | |
| Imbaraga z'Ingaruka | ≥100 J | |
Imiterere ya mekanike ni iyo hafi kandi ishobora gutandukana bitewe n'ubushyuhe, imyuka ikingira, ibipimo byo gusudira n'ibindi bintu.
Imyuka yo kurinda
EN ISO 14175 - TIG: I1 (Argon)
Imyanya yo gusudira
EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG
| Amakuru yo gupakira | |||
| Ingano | Uburebure | Uburemere | |
| mm 1.60 mm 2.40 mm 3.20 | mm 1000 mm 1000 mm 1000 | Ibiro 5 Ibiro 5 Ibiro 5 | |
Inshingano: Nubwo hakozwe ibishoboka byose kugira ngo amakuru ari muri ibyo abe ari ukuri, aya makuru ashobora guhinduka nta nteguza kandi ashobora gufatwa nk'akwiriye gusa nk'ubuyobozi rusange.