Insinga zo gusudira za Nickel Alloy Insinga za ERNiCrMo-4 Tig

Ibisobanuro bigufi:

ER-NiCrMo-4 ikoreshwa mu gusudira aloyi zifite imiterere isa ya shimi, harimo ibikoresho bitandukanye by’aloyi zikozwe muri nikeli, ibyuma n’ibyuma bitarangwamo ifu.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Aloyi ya nikeliInsinga zo gusudiraInsinga ya TigERNiCrMo-4

 

Amahame
EN ISO 18274 - Ni 6276 - NiCr15Mo16Fe6W4
AWS A5.14 – ER NiCrMo-4

 

Ibiranga na Porogaramu

ER-NiCrMo-4 ikoreshwa mu gusudira alloys zifite imiterere isa ya shimi, harimo n'ibikoresho bitandukanye byanikeli-ibyuma bikozwe mu byuma bikozwe mu buryo bw'ibanze, ibyuma n'ibyuma bitagira umugese.

Bitewe n'uko molybdenum irimo molekile nyinshi, iyi alloy itanga ubushobozi bwo kurwanya stress & corruption, corruption and scattering.

Ubusanzwe ikoreshwa ku miyoboro, ku mato y’umuvuduko, ku nganda zitunganya imiti, ku mbuga za peteroli zo mu nyanja, ku nganda zikora gaze, ku ngufu n’ibidukikije byo mu mazi n’ibindi.

Ibikoresho bisanzwe by'ibanze

N10276, W.Nr: 2.4819, NiMo16Cr15W, Aloyi C4, Aloyi C276*
* Urutonde rw'ibishushanyo, ntabwo ari urusobe rw'ibintu byose

 

 

Ibikubiye mu binyabutabire %
C% Mn% Fe% P% S% Si%  
umubare ntarengwa umubare ntarengwa umubare ntarengwa umubare ntarengwa umubare ntarengwa umubare ntarengwa  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Ko% Ti% Al%    
umubare ntarengwa 93.00 umubare ntarengwa 2.00 umubare ntarengwa    
0.20 umunota 1.00 3.50 1.00    

 

Imiterere ya mekanike
Imbaraga zo Gufata ≥690 MPa  
Imbaraga z'umusaruro -  
Kurekura -  
Imbaraga z'Ingaruka -  

Imiterere ya mekanike ni iyo hafi kandi ishobora gutandukana bitewe n'ubushyuhe, imyuka ikingira, ibipimo byo gusudira n'ibindi bintu.

 

Imyuka yo kurinda

EN ISO 14175 - TIG: I1 (Argon)

 

Imyanya yo gusudira

EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Amakuru yo gupakira
Ingano Uburebure Uburemere  
mm 1.60

mm 2.40

mm 3.20

mm 1000

mm 1000

mm 1000

Ibiro 5

Ibiro 5

Ibiro 5

 