AWS A5.20 E70T-7 Flux Cored Arc Welding Electrodes Flux Core Welding Wire

Ibisobanuro bigufi:

AWS A5.20 E70T-7 Flux Cored Arc Welding Wire ni insinga yikingira flux cored wire yagenewe gusudira cyane.Irakwiriye kumwanya uringaniye, utambitse kandi umanuka kuri DCEN polarite.


Ibicuruzwa birambuye

Ibicuruzwa

EN ISO 17632-KURI 42 ZW N 3

Ibiranga no kubishyira mu bikorwa
AWS A5.20 E70T-7AmashanyaraziArcWelding Wireni kwikingira-flux cored wire yagenewe gusudira cyane.Irakwiriye kumwanya uringaniye, utambitse kandi umanuka kuri DCEN polarite.Imikorere myiza cyane kuri X-ray igenzura, hamwe na desulfurasiyo bigabanya gucika mu gusudira amasahani manini, ingingo zifatanije hamwe nicyuma giciriritse.Ibisanzwe
Porogaramu ni ibihimbano rusange hamwe no gusudira muburyo aho gushira cyane hamwe no kwinjira neza kandi njye cyangwa umuvuduko wurugendo byihuse.Imyanya iboneka iringaniye, iringaniye kandi ihanamye hepfo yo gusudira kuri fllet weld hamwe na lap hamwe.

Imiti isanzwe igizwe na Weld Metal (%)
C 0.29 Mn 0.45 Si 0.10 P 0.010 S 0.005 AI 1.45

Ibikoresho bisanzwe bya mashini ya Weld Metal
Gutanga imbaraga 453Mpa Tensile Imbaraga 600MPa Kongera 25%

Inyandiko ku mikoreshereze:
1.DC (-) polarite irasabwa.
2. iyo ingaruka zikomeye zicyuma gisudira ni ngombwa.
3. Komeza ibicuruzwa byumye, mugihe bibitswe cyangwa byatanzwe.

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twagize uruhare mu gukora electrode yo gusudira,gusudira, no gusudira ibikoreshwa mu myaka irenga 20.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.