AWS A5.23: ECM1 Ikoreshwa mu gusudira insinga zo mu bwoko bwa Arc Welding

Ibisobanuro bigufi:

AWS A5.23: ECM1, Insinga ya Arc Cored Wire yo munsi y’amazi ni insinga y’icyuma ifite insinga nkeya ikoreshwa mu gusudira arc iri munsi y’amazi mu buryo bukomeye.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

AWS A5.23: ECM1, Insinga zirimo imiyoboro y'icyuma gito gikozwe mu cyuma gikozwe mu buryo bwa Arc Cored

ECM1 ni electrode y'insinga ifite insinga nkeya ikoreshwa mu gusudira arc munsi y'amazi mu buryo bukomeye. Kandi ihuye na chemistry ya AWS A5.23 M1 kandi yagenewe imbaraga zo gukurura zirenze 80 ksi.

IBIKORESHO N'INZUNGU
• Insinga zikozwe mu byuma zishobora gutanga igipimo cyiza cyo gushyiramo ugereranije n'insinga zikomeye ku buryo bungana na amperage
• Insinga zifite ibyuma zitanga imiterere yagutse y’ubwinjirire ugereranije n’insinga zikomeye ku bipimo byo gusudira bisa.
• Itanga ubukomezi bwiza cyane ku bushyuhe buri hasi haba mu bihe byasutsweho ndetse no mu bihe byo kugabanya stress.
• Ibisabwa ku miterere y'imiti yo gusukamo ubutare bisa n'iby'insinga zikomeye za EM1
• Bikwiriye gukoreshwa hamwe n'ubwoko bwinshi bw'imitsi
• Bitanga amahirwe yo kongera umuvuduko w'ingendo kugira ngo umusaruro urusheho kwiyongera
• Bifasha mu kwirinda gushya iyo usudira ku mirasire myinshi ku mizi y'amazi n'ibikoresho bito cyane.
• Bifasha kugabanya ibyago byo kwangirika mu bikorwa bikomeye cyangwa ahantu hakomeye hakorerwa serivisi
• Ikwiriye nk'uburyo bwo kongera umusaruro mu bikorwa byinshi ubu ikoresha insinga ikomeye ya EM1 (cyangwa 80 ksi isa nayo)
• Itanga uburyo butandukanye mu gutegura no kunoza imikorere y'ubusudizi

Inganda
Gukora inyubako n'ibiraro, ibikoresho biremereye, gutanga amashanyarazi, kubaka amato, n'ibindi bikoresho byo mu mazi
UBU
Electrode y'Umuriro Uziguye (DCEP), Electrode y'Umuriro Uziguye (DCEN), Umuriro Usimburana (AC)
UBUBIKO
Ibicuruzwa bigomba kubikwa ahantu humutse kandi hafungiye, kandi mu ipaki yabyo y'umwimerere imeze neza
INGINGO ZA AWS


  • Ibanjirije iyi:
  • Ibikurikira: