Ibisobanuro bigufi:

J507 (AWS E7015) ni electrode y'icyuma cya karuboni ifite irangi rike rya hydrogen sodium. Icyuma cyashyizwemo gifite plasticity nziza, gukomera, no kudacika kw'imivuniko.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira Icyuma cya KaruboniElectrode

J507

GB/T E5015

AWS A5.1 E7015

Ibisobanuro: J507 ni electrode y'icyuma cya karuboni ifite sodium nke ya hydrogen. Ibyuma byashyizwemo bifite plasticity nziza, gukomera, no kudacika kw'imivuniko. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse), kandi ishobora gusudira ahantu hose.

Ikoreshwa: Ikoreshwa mu gusudira ibyuma bipima karuboni n'ibindi byuma bipima karuboni nke, nka 09Mn2Si, Q345, 09Mn2V, nibindi.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

S

P

≤0.12

≤1.60

≤0.75

≤0.035

≤0.035

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Agaciro k'ingaruka (J)

-20℃

-30℃

Yemejwe

≥490

≥400

≥22

≥47

≥27

Byapimwe

520 ~ 580

≥410

24 ~ 32

60 ~ 230

55 ~ 200

 

Ingano ya hydrogen mu byuma byabitswe: ≤8.0mL/100g (uburyo bwa glycerin)

 

Isuzuma rya X-ray: Icyiciro cya mbere

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(cyangwa semm)

2.0

2.5

3.2

4.0

5.0

5.8

Umuyoboro wo gusudira

(cyangwa seA)

40~ 70

60 ~ 90

90 ~ 130

140 ~ 180

170 ~ 210

210~ 260

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe kuri dogere 350 mbere yo gusudira;

2. Ni ngombwa gusukura ingese, igipimo cy'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira;

3. Koresha uburyo bwo gusudira bugufi mu gihe usuka. Uburyo bwo gusudira buto bukwiye.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo electrode zo gusudira ibyuma bidashonga, electrode zo gusudira ibyuma bya karuboni, electrode zo gusudira zifite alloy low alloy, electrode zo gusudira hejuru, electrode zo gusudira za nickel na cobalt alloy, insinga zo gusudira zifite alloy low alloy, insinga zo gusudira zifite alloy steel, insinga zo gusudira zifite gazi, insinga zo gusudira za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nickel na cobalt alloy, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gusudira karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 


  • Ibanjirije iyi:
  • Ibikurikira: