E6010 electrode yo gusudira icyuma cya karuboni

Ibisobanuro bigufi:

E6010 ni electrode yo mu bwoko bwa rutile-cellulosic sodium.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira y'icyuma giciriritse cya AWS E6010

IBIKORESHO:

Ikwiriye gusudira ibyuma bifite imiterere mike ya karubone nk'imiyoboro, kubaka amato n'ikiraro n'ibindi.

IBIKORESHO BYA MBERE:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

IBIKORESHO:

E6010 ni electrode yo mu bwoko bwa rutile-cellulosic sodium. Ishobora gusudira ahantu hose (cyane cyane iyo iri mu mwanya uhagaze) hamwe na DC+ gusa. Ifite ubushobozi bwiza bwo gusudira kuko ifite umurambararo uhamye, itose gato, ikuraho ibintu byoroshye kandi ikagira ubushobozi bwo kongera imbaraga n'ibindi. Igenzura neza pisine ishongeshejwe, imbaraga zikomeye z'umurambararo no kwinjira byimbitse mu mwanya uhagaze.

IMITERERE Y'IBYUMA BYOSE BYO GUSUDURA: (UBUREBURE %)

Ibintu C Mn Si S P Ni Cr Mo V
Ibisabwa ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Ibisubizo bisanzwe 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

IMITUNGO Y'IBYUMA BYOSE BYO GUSHUSHANYA:

Ibintu Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Ibisabwa ≥430 ≥330 ≥20 ≥27
Ibisubizo bisanzwe 475 400 26 80

KWITONDA:

1. Muri rusange, ntugomba kongera kumisha electrode mbere yo kuyisudira. Iyo yangiritse ku bushyuhe, ugomba kongera kuyimisha kuri 70℃-90℃ mu gihe cy'isaha imwe.

2. Ingese, amavuta, amazi n'indi myanda yo mu gace karimo gusudira bigomba gukurwaho mbere yo gusudira.

UBURYO BUSANGE BWO GUKORA: (DC+)

Ingano (mm) 2.5 3.2 4.0 5.0
Uburebure (mm) 300 350 400 400
Umuvuduko w'amashanyarazi (A) 50-80 60-100 100-140 140-180

GUPIKA:

5kg/agasanduku, udusanduku 4/agasanduku, 20kg/agasanduku, udusanduku 50/agapaki. 21MT -26MT kuri 1X20″ FCL.

 

OEM/ODM:

Dushyigikiye OEM/ODM kandi dushobora gukora ipaki hakurikijwe imiterere yawe, turagusaba kutwandikira kugira ngo tuganire ku birambuye.

 

Ibiranga Imikoreshereze:

Umuheto uhamye cyane.

Gukuraho neza cyane ibisigazwa by'imyanda.

Kwinjira ni gake cyane.

Ubudahangarwa bwiza bw'ubushyuhe n'ingese.

Ubudahangarwa bwiza cyane bw'imipfundo.