AWS E7014 Amashanyarazi ya Carbone Amashanyarazi J501Fe Yoroheje yo gusudira ibyuma

Ibisobanuro bigufi:

J501Fe (AWS E7014) ni ifu yicyuma nubwoko bwa titanium oxyde itwikiriye electrode.


Ibicuruzwa birambuye

Ibicuruzwa

Amashanyarazi ya Carbone

J501Fe

GB / T E5014

AWS A5.1 E7014

Ibisobanuro: J501Fe ni ifu yicyuma nubwoko bwa titanium oxyde itwikiriye electrode.Irashobora gukoreshwa kumwanya wose wo gusudira hamwe na AC na DC, uburyo bwo kubitsa ni 110%.

Gushyira mu bikorwa: Kubyuma bya karubone hamwe nububiko buke bwibyuma, nka Q345 nandi mato, ibinyabiziga hamwe nubukanishi bwo gusudira.

Ibigize imiti yicyuma (%):

C

Mn

Si

S

P

≤0.12

≤1.25

60.60

≤0.035

≤0.035

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Agaciro k'ingaruka (J)

0 ℃

Bijejwe

90490

00400

≥17

≥27

Yageragejwe

520 ~ 580

≥410

17 ~ 26

50 ~ 100

 

Kugenzura X-ray: Icyiciro cya II

Icyifuzo kigezweho:

Diameter

(Mm)

2.0

2.5

3.2

4.0

5.0

5.8

Umuyoboro wo gusudira

A)

40 ~ 70

70 ~ 90

90 ~ 130

160 ~ 210

210 ~ 250

260 ~ 310

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka isaga 20 dukora umwuga wo gukora electrode yo gusudira, inkoni zo gusudira, hamwe n’ibikoresho byo gusudira.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.

 

 