AWS E6013 (J421X) Electrode yo gusudira mu byuma bya karuboni yo gusudira mu buryo buhagaze

Ibisobanuro bigufi:

J421X (AWS E6013) ni electrode ifite titanium nyinshi ikoreshwa mu gusudira icyuma cya karuboni.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira Icyuma cya KaruboniElectrode

J421X                                                      

GB/T E4313

AWS A5.1 E6013

Ibisobanuro: J421X ni electrode ifite titaniyumu nyinshi ikoreshwa mu gusudira icyuma cya karuboni. Ishobora gukora mu mwanya uhagaze, kandi ikwiriye gusudira ahantu hose hamwe n'imikorere myiza yo gusudira, kandi ishobora gukoreshwa kuri AC na DC. Sudi iraryoshye kandi iratunganye. Umugozi urahamye kandi woroshye kongera kuwukoresha, ibisigazwa bishobora gukurwaho byoroshye.

 Ikoreshwa: Ikoreshwa no gusudira icyuma cya karuboni n'icyuma cya galvanized, cyane cyane, isudira icyuma gito mu mwanya uhagaze no gusudira bidatinze.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

S

P

≈0.08

≈0.5

≈0.25

≤0.035

≤0.040

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Agaciro k'ingaruka (J)

Ubushyuhe Busanzwe.

0℃

Yemejwe

≥420

≥330

≥17

—

—

Byapimwe

460 ~ 540

370 ~ 420

≈25

≈80

≈70

 Isuzuma rya X-ray: Icyiciro cya II

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.0

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

50 ~ 70

60 ~ 100

80 ~ 150

160 ~ 200

180 ~ 250

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo icyuma kitagira umugeseelectrode yo gusudiras, electrode zo gusudira icyuma cya karuboni, electrode zo gusudira zifite alloy nkeya, electrode zo gusudira hejuru, electrode zo gusudira za nikeli na kobalti, insinga zo gusudira zifite icyuma gito n'alloy nkeya, insinga zo gusudira zifite icyuma kidafunze, insinga zikingira gazi, insinga zo gusudira za aluminiyumu, gusudira arc munsi y'amazi. insinga, insinga zo gusudira za nikeli na kobalti, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gukata karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 


  • Ibanjirije iyi:
  • Ibikurikira: