AWS E7018 Inkoni zo gusudira J506Fe Ifu Yicyuma Hasi ya Hydrogen Potasiyumu Electrode

Ibisobanuro bigufi:

J506Fe (AWS E7018) ni ifu yicyuma gito hydrogène potasiyumu electrode.Ikoreshwa kuri AC na DC mumyanya yose.


Ibicuruzwa birambuye

Ibicuruzwa

Amashanyarazi ya Carbone

J506Fe                                                  

GB / T E5018

AWS A5.1 E7018

Ibisobanuro: J506Fe ni ifu yicyuma hydrogène potasiyumu electrode.Ikoreshwa kuri AC na DC mumyanya yose.Nkuko igifuniko kirimo ifu yicyuma, ifite gusudira neza kandi irashobora kugabanya ibice byo gusudira.

Gushyira mu bikorwa: Ikoreshwa mu gusudira ibyuma bya karubone hamwe nicyuma giciriritse cyingero zingana zingana, nka Q345, nibindi.

 

Ibigize imiti yicyuma (%):

C

Mn

Si

S

P

≤0.12

601.60

≤0.75

≤0.030

≤0.035

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Agaciro k'ingaruka (J)

(-30 ℃)

Bijejwe

90490

00400

≥22

≥27

Yageragejwe

520 ~ 580

≥410

24 ~ 30

50 ~ 180

 

Diffusion hydrogène yibikoresho byabitswe: ≤8.0mL / 100g (uburyo bwa glycerine)

Igenzura rya X-ray: I amanota

 

Icyifuzo kigezweho:

Diameter

(Mm)

2.5

3.2

4.0

5.0

5.8

Umuyoboro wo gusudira

A)

90 ~ 120

120 ~ 150

170 ~ 200

210 ~ 250

240 ~ 310

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha 1 kuri 350 ℃ mbere yo gusudira;

2. Ni ngombwa guhanagura ingese, igipimo cyamavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira;

3. Koresha ibikorwa bigufi arc mugihe cyo gusudira.Inzira ifunganye yo gusudira irakwiriye.;

4. Huza electrode kuri pole nziza mugihe ikora kuri DC.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Tumaze imyaka isaga 20 dukora umwuga wo gukora electrode yo gusudira, inkoni zo gusudira, hamwe n’ibikoresho byo gusudira.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.

 