Electrode y'icyuma cya TYUE E6013 (J421X) ya karuboni

Ibisobanuro bigufi:

AWS A5.1 E6013(J421) ni electrode yo mu bwoko bwa rutile.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gushyira mu byiciro:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Ibiranga:

AWS A5.1 E6013(J421X) ni electrode yo mu bwoko bwa rutile. Ishobora gusudira haba isoko y'amashanyarazi ya AC na DC kandi ishobora gukoreshwa ahantu hose. Ifite imikorere myiza yo gusudira nk'umusego uhamye, imiyoboro mito, gukuraho ibintu byoroshye no kongera imbaraga n'ibindi. Electrode ya rutile-cellulosic ifite ubushobozi bwo gusudira neza mu myanya yose harimo no kumanuka mu buryo buhagaze. Ifite ubushobozi bwiza bwo guhuza icyuho no gukurura umusego. Ikoreshwa mu gusudira no gushyira imizigo mu buryo buhamye. Ikoreshwa muri rusange mu nganda n'ubucuruzi, guteranya no gusudira mu maduka.

Ibikoresho bya shimiby'ibyuma byose byasuwede:(%)
Ibikoresho bya shimi C Mn Si S P Ni Cr Mo V
Ibisabwa ≤0.10 0.32-0.55 ≤0.30 ≤0.030 ≤0.035 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Ibisubizo bisanzwe 0.08 0.37 0.18 0.020 0.025 0.030 0.035 0.005 0.004
Imiterere ya tekiniki y'ibyuma byabitswe
Ikintu cy'igerageza Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Ibisabwa 440-560 ≥355 ≥22 ≥47
Ibisubizo bisanzwe 500 430 27 80
Ikoreshwa ry'Umuyoboro w'Ifatizo (DC)
Ingano φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 80~ 130 150 ~ 210 180 ~ 240

Aho gusudira:

PA, PB, PC, PD, PE, PF

Isuzuma rya X-Ray Radiographic:

UrwegoⅡ

Icyitonderwa:

Muri rusange, ntugire'Ntugomba kongera kumisha electrode mbere yo kuyisudira. Iyo igize ikibazo cy'ubushuhe, ugomba kongera kuyimisha kuri dogere 150.℃-170℃mu gihe cy'isaha 0.5-1.