E316L-16 Electrode y'icyuma kidafunze

Ibisobanuro bigufi:

E316L-16 Gusudira karubone nkeya cyane 18%Cr-12%Ni-2%Mo (icyuma kitagira umugese cya 316L)


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

AWS A5.4 E316L-16 Inkingi zo gusudira mu byuma bitagira umwanda

AWS: SFA 5.4 E316L-16

IS: 5206 E19.12.2.LR16

EN ISO CODE: 3581-AE 19 12 3 LR 3 2

Ibiranga Imikoreshereze:

E316L-16 ni electrode yo mu bwoko bwa lime-titania ifite ubushobozi bwo gukoresha neza no gusudira.

Kubera ko icyuma cyometseho byose gifite imiterere ya austenite irimo ingano ikwiye ya ferrite, ubushobozi bwo guhangana n'impinduka ni bwiza. Gifite ubushobozi bwo guhangana n'impinduka za intercrystalline mu gihe cyometseho kuko ingano ya karuboni ari nke kandi ubushobozi bwo guhangana n'impinduka za intergranular buruta ubwa E316L-16 kandi gifite Mo. Ubushobozi bwo guhangana n'ubushyuhe nabwo ni bwiza.

E316L-16 ifite ubushobozi bwo kurwanya ubushuhe bwinshi kandi ikagira ubushobozi bwo kurwanya imirasire.

IMITERERE Y'IBYUMA BYOSE BYO GUSUDURA (%)

Igice

C

Mn

Si

Cr

Ni

Mo

S

P

Cu

Ijanisha

≤0.04

0.50-2.50

≤0.90

17-22

11-14

2.0-3.0

≤0.030

≤0.04

≤0.75

IMITUNGO Y'IBYUMA BYOSE BYO GUSHUSHANYA

UTS

Kurekura

(MPa)

(L= 5d)%

545

40

AMAKURU Y'UBU N'AYO GUPAKIRA: AC / DC(+)

Ingano (mm)

5×350

4×350

3.15×350

2.5×350

Ingano y'Ubu (Amps)

150-180

110-140

80-100

60-80

Uburemere / Ikarito (kgs)

2.5

2.5

2.5

2.5

Kwitonda:

1. Koresha umugozi mugufi n'agasaro k'imigozi kugira ngo ugabanye ubushyuhe bwinjira.

2. Menya neza ko electrode zumutse. Ongera wumishe electrode kuri dogere selisiyusi 250-300 mu gihe cy'isaha imwe.

Ibisobanuro ku ikoreshwa:

Ubugari bwo kuboha bugomba kuba munsi y'umurambararo wa electrode inshuro ebyiri n'igice.

Kuraho imyanda nk'amavuta n'umukungugu mu mwobo.

Shyira electrodes kuri dogere 350 (662) mu gihe cy'iminota 60 mbere yo kuyikoresha.