AWS E317L-16 Icyuma Cyuma Cyuma Cyuma Cyuma Cyuma Cyuma,

Ibisobanuro bigufi:

A032Mo (AWS E317L-16) ni karubone ntoya cyane ya karubone Cr19Ni13Mo3 ibyuma bitagira umuyonga electrode hamwe na calcium ya calcium ya titanium.


Ibicuruzwa birambuye

Ibicuruzwa

Gusudira ibyumaElectrode

A032Mo                                            

GB / T E317L-16

AWS E317L-16

Ibisobanuro: A032Mo ni ultra-nkeya ya karubone Cr19Ni13Mo3 ibyuma bitagira umuyonga electrode hamwe na calcium ya calcium ya titanium.Irashobora gukoreshwa kuri AC na DC hamwe nibikorwa byiza.Kurwanya ruswa irwanya aside sulfurike, aside sulfure na aside kama iruta iya E316L.

Gushyira mu bikorwa: Ikoreshwa mu gusudira ubwoko bumwe bwibikoresho bidafite ingese nka AISI317 na 317L ibyuma, kandi biranakenewe mu gusudira no kugaragara hejuru yangirika kwangirika kwibyuma hamwe nibyuma bidasanzwe.

 

Ibigize imiti yicyuma (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

90.90

18.0 ~ 21.0

12.0 ~ 14.0

3.0 ~ 4.0

≤0.75

≤0.030

.040.040

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Kurambura

%

Bijejwe

20520

≥25

 

Icyifuzo kigezweho:

Diameter

(Mm)

2.0

2.5

3.2

4.0

5.0

Kuzenguruka

A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 220

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha 1 hafi 250 ℃ mbere yo gusudira;

2. Ni ngombwa guhanagura ingese, igipimo cyamavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira.

 

Wenzhou Tianyu Electronic Co., Ltd yashinzwe mu 2000. Twagize uruhare mu gukoragusudira electrodes, gusudira, nagusudiraimyaka irenga 20.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.


  • Mbere:
  • Ibikurikira: