AWS E7015-G Electrode yo Gusudira mu Cyuma gishyuha cyane W607 Inkoni yo Gusudira ifite Hydrogen nkeya

Ibisobanuro bigufi:

W607 (AWS E7015-G) ni electrode y'icyuma ikoresha ubushyuhe buke ifite irangi rito rya hydrogen sodium


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira mu byuma bishyuha cyane

W607                                                     

GB/T E5015-G

AWS A5.5 E7015-G

 

Ibisobanuro: W607 ni electrode y'icyuma ifite ubushyuhe buke ifite sodium nkeya ya hydrogen. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse) kandi ishobora gusudira ahantu hose. Icyuma cyashyizwemo gifite ubukana bwiza kuri -60°C.

Ikoreshwa: Ikoreshwa mu gusudira ibyuma bifite ubushyuhe buke nka 09MnD.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Ni

S

P

≤0.08

≤1.65

≤0.60

0.50 ~ 2.50

≤0.020

≤0.025

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Agaciro k'ingaruka (J)

-60℃

Yemejwe

≥490

≥390

≥22

≥27

 

Ingano ya hydrogen mu byuma byabitswe: ≤6.0mL/100g (uburyo bwa glycerin) cyangwa ≤10mL/100g (uburyo bwa mercury cyangwa gas chromatography)

Isuzuma rya X-ray: Icyiciro cya mbere

 

Ikoreshwa ry'amashanyarazi risabwa:

(mm)

Umwanya w'inkoni

2.0

2.5

3.2

4.0

5.0

(A)

Umuyoboro wo gusudira

40 ~ 70

60 ~ 90

100 ~ 120

140 ~ 170

170 ~ 200

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe kuri dogere 350 mbere yo gusudira;

2. Ni ngombwa gusukura ingese, igipimo cy'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira;

3. Igice gisutswe gishobora gushyuha cyane ku bushyuhe bwa dogere selisiyusi 150 mbere yo gusudira kugira ngo hirindwe ko hacikamo ibice.

 


  • Ibanjirije iyi:
  • Ibikurikira: