W707Ni ni electrode yubushyuhe buke burimo Ni muburyo bwa hydrogène sodium.


Ibicuruzwa birambuye

Ibicuruzwa

Ubushyuhe bukeGusudiraElectrode

W707Ni                                                     

GB / T E5515-C1

Ibisobanuro: W707Ni ni electrode yubushyuhe buke burimo Ni muri sodium ya hydrogène nkeya.Koresha DCEP (itaziguye ya electrode nziza) kandi irashobora gusudira mumyanya yose.Icyuma cyabitswe kiracyafite ingaruka nziza kuri -70 ° C.

Gusaba: Byakoreshejwe mu gusudira ubushyuhe buke nka 2.5Ni.

 

Ibigize imiti yicyuma (%):

C

Mn

Si

Ni

S

P

≤0.12

≤1.25

60.60

2.00 ~ 2.75

≤0.020

≤0.025

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Agaciro k'ingaruka (J)

-70 ℃

Bijejwe

40540

40440

≥17

≥27

 

Diffusion hydrogène yibikoresho byabitswe: ≤6.0mL / 100g (uburyo bwa glycerine) cyangwa ≤10mL / 100g (uburyo bwa mercure cyangwa gaz chromatografiya)

Igenzura rya X-ray: I amanota

 

Icyifuzo kigezweho:

(Mm)

Diameter

2.0

2.5

3.2

4.0

5.0

A)

Kuzenguruka

40 ~ 70

60 ~ 90

90 ~ 120

140 ~ 180

170 ~ 210

 Icyitonderwa:

  1. Electrode igomba gutekwa kumasaha 1 kuri 350 ℃ mbere yo gusudira;
  2. Ni ngombwa guhanagura ingese, igipimo cyamavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira;
  3. Gerageza gukoresha umurongo muto imbaraga mugihe cyo gusudira, ibyiciro byinshi hamwe no gusudira byinshi.

 