Electrode yo gusudira y'icyuma ya AWS E8015-G yo hasi ya hydrogen

Ibisobanuro bigufi:

J557 (AWS E8015-G) ni electrode y'icyuma ifite aloyi nkeya ifite sodium nkeya ya hydrogen. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse), kandi ishobora gusukurwa ahantu hose.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Electrode yo gusudira y'icyuma gikozwe mu cyuma gito

J557                                             

GB/T E5515-G

AWS E8015-G

Ibisobanuro: J557 ni electrode y'icyuma ifite aloyide nkeya ifite sodium nkeya ya hydrogen. Koresha DCEP (electrode y'umuyoboro w'amashanyarazi ugororotse), kandi ishobora gusukurwa ahantu hose.

Ikoreshwa: Ikoreshwa mu gusudira ibyuma bipima karuboni n'ibyuma bipima aloyi nke nka Q390.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

S

P

≤0.12

≥1.00

0.30 ~ 0.70

≤0.035

≤0.035

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Agaciro k'ingaruka (J)

-20℃

-30℃

Yemejwe

≥540

≥440

≥17

—

≥27

 

Ingano ya hydrogen mu byuma byabitswe: ≤6.0mL/100g (uburyo bwa glycerin)

Isuzuma rya X-ray: Icyiciro cya mbere

 

Ikoreshwa ry'amashanyarazi risabwa:

(mm)

Umwanya w'inkoni

2.5

3.2

4.0

5.0

(A)

Umuyoboro wo gusudira

60 ~ 90

80 ~ 110

130 ~ 170

160 ~ 200

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe ku bushyuhe bwa 350°C mbere yo gusudira;

2. Ni ngombwa gusukura ingese, igipimo cy'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira;

3. Koresha uburyo bwo gusudira bugufi mu gihe usuka. Uburyo bwo gusudira buto bukwiye.

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, n'ibikoresho byo gusudira mu gihe cy'imyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo icyuma kitagira umugeseelectrode yo gusudiras, electrodes zo gusudira ibyuma bya karuboni,electrode zo gusudira zifite alloy nkeya, electrode zo gusudira hejuru, electrode zo gusudira za nikeli na kobalti, insinga zo gusudira z'icyuma gito n'icyuma gito, insinga zo gusudira z'icyuma kitagira umugese, insinga zikingira gazi, insinga za aluminiyumu, insinga zo gusudira zicukuwe. insinga, insinga zo gusudira za nikeli na kobalti, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gukata karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.

 


  • Ibanjirije iyi:
  • Ibikurikira: