AWS E8018-C1 Electrode yo gusudira mu byuma bishyuha cyane W606Fe Hydrogen nkeya ARC Welding Rods

Ibisobanuro bigufi:

W606Fe (AWS E8018-C1) ni electrode y'icyuma ikoresha ubushyuhe buke ifite ifu y'icyuma n'igipfundikizo gito cya hydrogen potasiyumu


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Ubushyuhe buri hasiGusudira mu byumaElectrode

W606Fe                                                     

GB/T E5518-C1

AWS A5.5 E8018-C1

Ibisobanuro: W606Fe ni electrode y'icyuma ikoresha ubushyuhe buke ifite ifu y'icyuma n'igitambaro gito cya hydrogen potasiyumu. Ishobora gukoreshwa mu gusudira ahantu hose hakoreshejwe AC na DC. Icyuma cyashyizwemo gifite ubukana bwiza kuri -60°C. 

Ikoreshwa: Ikoreshwa mu gusudira ibyuma bifite ubushyuhe buke nka 2.5Ni.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Ni

S

P

≤0. 12

≤1.25

≤0.80

2.00 ~ 2.75

≤0.020

≤0.025

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

Imbaraga zo gukurura

Mpa

Imbaraga z'umusaruro

Mpa

Kurekura

%

Agaciro k'ingaruka (J)

-60℃

Yemejwe

≥540

≥440

≥17

≥27

 

Ingano ya hydrogen mu byuma byabitswe: ≤6.0mL/100g (uburyo bwa glycerin) cyangwa ≤10mL/100g (uburyo bwa mercury cyangwa gas chromatography)

Isuzuma rya X-ray: Icyiciro cya mbere

 

Ikoreshwa ry'amashanyarazi risabwa:

(mm)

Umwanya w'inkoni

3.2

4.0

5.0

(A)

Umuyoboro wo gusudira

90 ~ 120

140 ~ 180

180 ~ 210

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe kuri dogere 350 mbere yo gusudira;

2. Ni ngombwa gusukura ingese, ibipimo by'amavuta, amazi, n'imyanda ku bice byo gusudira mbere yo gusudira.

 


  • Ibanjirije iyi: