AWS E9015-G Amashanyarazi make yo gusudira Amashanyarazi yo hasi ya hydrogène yo gusudira Electrode J607CrNiMo

Ibisobanuro bigufi:

J607CrNiMo (AWS E9015-G) ni electrode ya elegitoronike ntoya hamwe na hydrogène sodium nkeya.


Ibicuruzwa birambuye

Ibicuruzwa

Amashanyarazi make yo gusudira Electrode

J607CrNiMo                                       

GB / T E6015-G

AWS E9015-G

 

Ibisobanuro: J607CrNiMo ni electrode nkeya ya elegitoronike ya elegitoronike hamwe na sodium ya hydrogène nkeya.Koresha DCEP (itaziguye ya electrode nziza), kandi irashobora gusudira mumyanya yose hamwe nibikorwa bigufi arc.Inkoni yo gusudira ifite uburebure bwimbitse, butagabanije kandi bukora neza.Ibyuma byabitswe bifite plastike nziza, ubukonje buke no kurwanya ibice.

Gushyira mu bikorwa: Ikoreshwa mu gusudira imiyoboro itanga amazi munsi ya 350 ° C muri sitasiyo y’amashanyarazi hamwe nicyuma cyumuvuduko cyingero zingana.Ifite umukino mwiza hamwe nicyuma cya WB36CN1 (HD15Ni1MnMoNbCu), kandi irakwiriye no gusudira ibyuma bya WB3 (15NiCuMoNb5).

 

Ibigize imiti yicyuma (%):

C

Mn

Si

Cr

Ni

Mo

S

P

≤0.10

1.00 ~ 1.60

≤0.50

0.14 ~ 0.35

0.60 ~ 1.20

0.15 ~ 0.50

≤0.015

≤0.015

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Agaciro k'ingaruka (J)

-30 ℃

Bijejwe

620 ~ 720

00500

≥20

≥47

 

Diffusion hydrogène yibikoresho byabitswe: ≤5.0mL / 100g (uburyo bwa mercure cyangwa gaz chromatografiya)

Igenzura rya X-ray: I amanota

 

Icyifuzo kigezweho:

(Mm)

Diameter

3.2

4.0

5.0

A)

Kuzenguruka

100 ~ 140

140 ~ 18

190 ~ 230

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha 1 hafi 350 ℃ mbere yo gusudira;

2. Ni ngombwa guhanagura ingese, igipimo cyamavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira.