AWS ECuSi UmuringaIbikoresho bya elegitoronike Yashizwemo Electrode T207 Arc Umuringa Wibiti byo gusudira

Ibisobanuro bigufi:

T207 (AWS ECuSi) ni electrode y'umuringa hamwe n'umuringa wa silicon bronze hamwe na sodium ya hydrogène nkeya.


Ibicuruzwa birambuye

Ibicuruzwa

Umuringa n'umuringa Alloy Welding Electrode

T207                                                     

GB / T ECuSi-B

AWS A5.6 ECuSi

 

Ibisobanuro: T207 ni electrode y'umuringa hamwe na silicon bronze ya bronze hamwe na sodium ya hydrogène nkeya.Koresha DCEP (itaziguye ya electrode nziza) hamwe nibikoresho bikomeye bya mashini.Ifite ruswa irwanya aside irike itari acide ya nitric, aside nyinshi kama ninyanja.

 

Gushyira mu bikorwa: Birakwiriye gusudira umuringa, umuringa wa silikoni n'umuringa, gusudira hejuru y'imirongo y'imashini zikoresha imiti, n'ibindi.

 

Ibigize imiti yicyuma (%):

Cu

Si

Mn

Pb

Al + Ni + Zn

> 92.0

2.5 ~ 4.0

≤3.0

≤0.02

≤0.50

 

 

Ibikoresho bya tekinike yicyuma gisudira:

试验 项目

Ikizamini

抗拉强度

Imbaraga

Mpa

延伸 率

Kurambura

%

保证 值

Bijejwe

70270

≥20

 

 

Icyifuzo kigezweho:

Diameter

(Mm)

3.2

4.0

5.0

Kuzenguruka

A)

90 ~ 130

110 ~ 160

150 ~ 200

 

Icyitonderwa:

Icyitonderwa:

1. Electrode igomba gutekwa nka 300 ° C mumasaha 1 kugeza 2 mbere yo gusudira;

2. Ubushuhe, amavuta, okiside nindi myanda hejuru yubudodo bigomba kuvaho mbere yo gusudira.

3. Iyo gusudira umuringa wa silicon cyangwa kugaragara gusudira ku byuma, nta bushyuhe bukenewe.Ubushyuhe bwo gushyushya umuringa usukuye ni nka 450 ° C, n'ubushyuhe bwo gushyushya imiringa ni 300 ° C;

4. Gusudira bigufi-arc bigomba gukoreshwa mugihe cyo gusudira.Mugihe cyo gusudira-ibice byinshi, icyapa kiri hagati yabyo kigomba kuba

yakuweho burundu;nyuma yo gusudira, inyundo isudira hamwe ninyundo yo mumutwe kugirango itunganyirize ibinyampeke, ikureho imihangayiko, kandi wongere imbaraga na plastike ya weld.