Ibisobanuro bigufi:

D237 (B-84) ni electrode yo gutwikira cyane kumashanyarazi hamwe nicyuma cya karubone.Amasaro afite ubuso bunoze, butarimo ibice na pore, ubike ibintu bikomeye birwanya kwangirika ningaruka zo hagati.Biroroshye gusudira mumyanya yose usibye guhagarikwa hasi.


Ibicuruzwa birambuye

Ibicuruzwa

Gukomera kwa Welding Stick ElectrodeRODO P.

UMURINZI WA ARA RECUBRIMIENTO

Andika No.: D237 (B-84) 

Isesengura ry'ibyuma byabitswe (Indangagaciro zisanzwe)

C

Mn

Si

Cr

Mo

V

0.5%

0.3%

0.7%

7%

0.5%

0.5%

 

Ibiranga:

B- 84 ni electrode yo gutwikira cyane kumashanyarazi hamwe nicyuma cya karubone.Amasaro afite ubuso bunoze, butarimo ibice na pore, ubike ibintu bikomeye birwanya kwangirika ningaruka zo hagati.Biroroshye gusudira mumyanya yose usibye guhagarikwa hasi.

Ibikoresho bya mashini:Gukomera kuva 55 kugeza 60 HRc (ya layers)

Imyanya yo gusudira:Flat, Horizontal, Hejuru, Ihagaritse Hejuru.

 

Ibiriho na Polarite:

Kubisimburana cyangwa bitaziguye

Electrode kuri pole nziza

ø mm

ø in

Amperage

3.20

1/8

100-130

4.00

5/32

120-160

5.00

16/2

180-220

 

Gusaba: • Nibyiza byo gusubiramo ibikoresho bya kariyeri, gutwara, gucukura

• Kumurika imizingo

• Gukora imashini

• Imashini zigenda kwisi

• Icyuma cyogoshesha.

 

UBURENGANZIRA: 350mm.

URUPAPURO RWA BURUNDU: kg 20 / ibiro 44.

 

Wenzhou Tianyu Electronic Co., Ltd yashinzwe mu 2000. Twagize uruhare mu gukoragusudira electrodes, gusudira, no gusudira ibikoreshwa mu myaka irenga 20.

Ibicuruzwa byacu byingenzi birimo electrode yo gusudira ibyuma, ibyuma bya karuboni yo gusudira electrode, electrode nkeya yo gusudira, electrode igaragara hejuru ya elegitoronike, nikel & cobalt alloy welding electrode, ibyuma byoroheje & insinga zo gusudira ibyuma, insinga zidafite ingese, insinga zo gusudira aluminium, gusudira arc gusudira.insinga, nikel & cobalt alloy welding insinga, insinga zo gusudira imiringa, insinga zo gusudira TIG & MIG, electrode ya tungsten, electrode ya karubone, nibindi bikoresho byo gusudira & ibikoreshwa.

 

 

 

 


  • Mbere:
  • Ibikurikira: