Welding Abaguzi Batanga EM14KS Yashizwemo Arc Welding Wire, Carbone Steel Rods yo Kuzenguruka Arc Welding

Ibisobanuro bigufi:

EM14KS ni icyuma gisize, icyuma cya karubone electrode yo gusudira arc yarohamye.


Ibicuruzwa birambuye

Ibicuruzwa

EM14KS ni icyuma gisize, icyuma cya karubone electrode yo gusudira arc yarohamye.Yagenewe kumurongo umwe kandi myinshi yo gusudira karubone, hamwe na aliyumu yo hasi, ibyuma mumirongo iringaniye kandi itambitse.Hitamo EM14KS ikubiyemo inyongera ntoya ya titanium itezimbere ibyuma bisudira kandi bigafasha kugumana imbaraga nyuma yo kugabanya imihangayiko.Iyi electrode igomba gukoreshwa mu gusudira arc gusudira gusa.

GUKURIKIRA:

EC1 kuri AWS A5.17, SFA 5.17.

IMITERERE:

Hitamo EM14KS yagenewe gukora chimie yo kubitsa isudira ihwanye niyakozwe ninsinga zikomeye, EM14K electrode.Igishushanyo mbonera cyibisubizo bivamo igipimo cyinshi cyo guta kuruta insinga zikomeye iyo zikoreshwa kurwego rumwe.

Hitamo EM14KS itanga uburyo bwiza bwo kugenzura amasaro kuruta insinga zikomeye.Uburyo bwo kwinjira kuri electrode ifite amabara ni ngari kandi ntoya, bigabanya ubushake bwo gutwikwa binyuze mumizi cyangwa guhuza neza ingingo.

GUSABA:

Hitamo EM14KS nibyiza kubyo gusaba birimo gusudira imiyoboro yumuvuduko hamwe nicyuma cya karubone cyubatswe nka A36, A285, A515, na A516.Igomba gukoreshwa hamwe na flux idafite aho ibogamiye kandi irashobora gusimburwa ahantu hose insinga ikomeye, EM14K electrode irakoreshwa.

TIMPICAL DEPOSIT CHEMISTRY:

Wt%

C

Mn

P

S

Si

Ti

.06

1.55

.015

.015

.55

.05

BASABWE PARAMETERS WELDING:

5/64 ”

Amps
250

Volts
26-27

WFS (ipm)
90

ESO (muri)
¾ ”-1¼”

Igipimo cyo kubitsa (lb / hr)
6.5

350

29-30

160

11

500

33-34

290

20

3/32 ”

275

28-29

80

1 ”-1¼”

8.5

450

32-33

155

15.5

600

37-38

245

24.7

1/8 ”

400

28-29

68

1 ”-1¼”

11.5

550

32-33

100

17

750

37-38

150

26.5

5/32 ”

425

30-31

45

1¼ ”-1½”

11.5

650

34-35

80

18.5

900

40-42

140

38