AWS ER5183 Aluminium Welding Wire Aluminium MIG gusudira Rods Tig Wire

Ibisobanuro bigufi:

ER5183 ikwiranye na MIG gusudira aluminium magnesium ivanze ko imbaraga zisabwa zingana kandi niba icyuma fatizo ari 5083 cyangwa 5654 imbaraga za tensile zaba nyinshi cyane.Irakoreshwa cyane mugusudira aluminium magnesium alloy yubatswe yubwato, urubuga rwo hanze, lokomoteri & gare, ibinyabiziga bifite moteri, kontineri, imiyoboro ya kirogenike nibindi.


Ibicuruzwa birambuye

Ibicuruzwa

ER5183 ikwiranye na MIG gusudira aluminium magnesium ivanze ko imbaraga zisabwa zingana kandi niba icyuma fatizo ari 5083 cyangwa 5654 imbaraga za tensile zaba nyinshi cyane.Irakoreshwa cyane mugusudira aluminium magnesium alloy yubatswe yubwato, urubuga rwo hanze, lokomoteri & gare, ibinyabiziga bifite moteri, kontineri, imiyoboro ya kirogenike nibindi.Icyuma cyacyo gisudira gifite imbaraga zo kurwanya ruswa.

Umwanya wo gusudira: F, HF, V.

Ubwoko bwa none: DCEP

ICYITONDERWA:

Kugumana pake yinsinga mumeze neza mbere yo gusudira.

Ubuso bwombi bugomba gusudwa no gusudira hamwe ninsinga bigomba guhanagurwaho umwanda wanduye wamavuta, gutwika oxyde, ubushuhe nibindi.

Kugirango ubone isura nziza yo gusudira ni ngombwa gushyushya icyuma fatizo kugeza 100 ℃ -200 ℃ mbere yo gusudira niba ubunini bwacyo ari 10mm cyangwa burenga.

Nibyiza gushira subplate munsi ya weld kugirango utere ibyuma bishongeshejwe kugirango wizere ko byinjira muri weldment.

Ukurikije imyanya yo gusudira hamwe nubunini bwibyuma fatizo bigomba guhitamo gazi itandukanye, nka 100% Ar, 75% Ar + 25% He, 50% Ar + 50% He, nibindi.

Imiterere yo gusudira yavuzwe haruguru kugirango ikoreshwe gusa kandi nibyiza gukora ibyangombwa byo gusudira ukurikije umushinga mbere yo kubishyira muburyo bwo gusudira.

ER5183 CHIMICAL COMPOSITION YUBUMWE BWA DEPOSITED (%):

SI FE CU MN MG CR ZN TI AI BE
Bisanzwe ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 Kuringaniza ≤0.0003
Ibisanzwe 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 Kuringaniza 0.0001

UMUTUNGO W'IKORANABUHANGA W'UBUNTU BWA DEPOSITED (AW):

IMBARAGA ZA TENSILE RM (MPA) YIELD IMBARAGA REL (MPA) KUBONA A4 (%)
Ibisanzwe 280 150 18

Ingano & Basabwe Ibigezweho kuri MIG (DC +):

WELDING WIRE DIAMETER (MM) 1.2 1.6 2.0
Kuzenguruka (A) 180-300 200-400 240-450
Umuvuduko wo gusudira (V) 18-28 20-20 22-34

SIZES & BASABWE KUBONA TIG (DC¯):

WELDING WIRE DIAMETER (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Kuzenguruka (A) 150-250 200-320 220-400