ERNiFe-CI Nickel Alloy Welding Wire Tig Filler Rod Mig na Tig Welding Rods

Ibisobanuro bigufi:

ERNiFe-CI ikoreshwa mugusudira ibyuma.Iki cyuma cyuzuza gikoreshwa cyane kugirango gipfundikire ibyuma.Irakoreshwa kandi mugusana casting.Ubushyuhe bwa preheat na interpass ya 175ºC (350ºF) byibuze birasabwa mugihe cyo gusudira, bitabaye ibyo uturere twa weld hamwe nubushyuhe bishobora gutera ibice.


Ibicuruzwa birambuye

Ibicuruzwa

ERNiFe-CI ikoreshwa mugusudira ibyuma.Iki cyuma cyuzuza gikoreshwa cyane kugirango gipfundikire ibyuma.Irakoreshwa kandi mugusana casting.Ubushyuhe bwa preheat na interpass ya 175ºC (350ºF) byibuze birasabwa mugihe cyo gusudira, bitabaye ibyo uturere twa weld hamwe nubushyuhe bishobora gutera ibice.

Ni 55 (AWS icyiciro ntigisobanuwe) ni izina rya 55% Nickel wire.Ibiri munsi ya Nickel bituma iyi mavuta irushaho kugira ubukungu kurusha Ni 99. Kubitsa gusudira mubisanzwe birashobora gukoreshwa nimashini, ariko mugihe ibintu bivanze cyane, gusudira birashobora gukomera kandi bigoye gukora imashini.Bikunze gukoreshwa mugusana casting hamwe nibice biremereye cyangwa binini.Ugereranije na Ni 99, gusudira bikozwe na 55 Ni birakomeye kandi birahindagurika, kandi byihanganira fosifori muri casting.Ifite kandi coefficient yo hasi yo kwaguka kuruta Ni 99, bivamo imirongo mike yo guhuza.

UMURIMO W'IMIKORESHEREZE:

NickelNi45.0-60.0%

Uburinganire

SiliconSimax 4.0%

ManganeseMn2.5%

UmuringaCu2.5%

CarbonCmax 2.0%

AluminiumAlmax 1.0%

UMUTUNGO W'IKORANABUHANGA:

Imbaraga zingana Rm (MPa) Gutanga umusaruro Rp0.2 (MPa) Kurambura A%
min.393-579 (57-84 psi) 296-434 (40-64 psi) 6-13

IBIKORWA BY'ibicuruzwa:

Ibicuruzwa

Diameter, mm

Uburebure, mm

Umugozi wo gusudira MIG / GMAW

0.8, 1.0, 1.2, 1.6, 2.0, 2.4, 2.5, 3.2

-

Inkoni zo gusudira TIG / GTAW

2.0, 2.5, 3.2, 4.0, 5.0

915 - 1000

Umugozi wo gusudira SAW

2.0, 2.4, 3.2, 4.0, 5.0

-

Umuyoboro wa electrode

2.0, 2.5, 3.20, 3.25, 4.0, 5.0

250, 300, 350, 400, 450, 500

GUSABA:

Binary Nickel-Iron (Ni-Fe) na Ni ishingiye ku gusudira ibinini bitangwa mu gusudira hamwe ninsinga muburebure busanzwe cyangwa uburebure kugeza kubisabwa nabaguzi.Kubintu bisanzwe bya serivise, imiti yimiti iraboneka mubintu bitandukanye Ni ukurikije ibipimo byinshi byabanyamerika nu Burayi.