Nickel na Nickel Alloy Welding Electrode AWS A5.11 ENiCrFe-7 Hydrogen Ntoya Nickel Welding Rods, Inkoni yo gusudira Arc

Ibisobanuro bigufi:

Ni307-7 (ENiCrFe-7) ni electrode ishingiye kuri nikel ifite sodium ya hydrogène nkeya.Koresha DCEP (itaziguye ya electrode nziza).


Ibicuruzwa birambuye

Ibicuruzwa

Nickel na Nickel Alloy Welding Electrode

Ni307-7                                                     

GB / T ENi6152

AWS A5.11 ENiCrFe-7

 

Ibisobanuro: Ni307-7 ni electrode ishingiye kuri nikel hamwe na sodium ya hydrogène nkeya.Koresha DCEP (electrode igezwehobyiza).Ifite imikorere myiza yo gusudira hamwe na arc ihamye, gutwika gake, gukuramo byoroshye,na weld nziza.Icyuma cyabitswe gifite imiterere ihamye kandi irwanya ruswa muriubushyuhe bwo hejuru bwa okiside hamwe nikirere kirimo sulfure.

 

Gushyira mu bikorwa: Byakoreshejwe mu buhanga bwa kirimbuzi, aside sulfurike, aside nitricike n’ibikoresho byo gukora fluor ya hydrogène, nka nikel 690 alloy, ASTM B166, B167, b168, nibindi, birashobora kandi gukoreshwa mugusudira nikel-chromium ibyuma nicyuma kitagaragara kandi cyangirika. -ibice bitarwanya ibyuma.

 

Ibigize imiti yicyuma (%):

C

Mn

Fe

Si

Ni

Cr

≤0.05

≤5.0

7.0 ~ 12.0

≤0.8

≥50.0

28.0 ~ 31.5

Cu

Mo

Nb

S

P

Ibindi

≤0.5

≤0.5

1.0 ~ 2.5

≤0.015

≤0.020

≤0.5

 

Ibikoresho bya tekinike yicyuma gisudira:

Ikizamini

Imbaraga

Mpa

Tanga imbaraga

Mpa

Kurambura

%

Bijejwe

50550

60360

≥27

 

Icyifuzo kigezweho:

Diameter

(Mm)

2.5

3.2

4.0

Umuyoboro wo gusudira

A)

60 ~ 90

80 ~ 110

110 ~ 150

 

Icyitonderwa:

1. Electrode igomba gutekwa kumasaha1 hafi 300 ℃ mbere yo gusudira;

2. Ni ngombwa guhanagura ingese, amavuta, amazi, n’umwanda ku bice byo gusudira mbere yo gusudira.Gerageza gukoresha arc ngufi kugirango usudire.

 

 