Ama-electrode yo gusudira mu byuma bitagira umugese AWS E308-15 afite irangi rito rya hydrogen

Ibisobanuro bigufi:

A107 (AWS E308-15) ni electrode y'icyuma kitagira umukungugu ya Cr19Ni10 ifite karubone nkeya ifite sodiyumu nkeya.


Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

Gusudira mu byuma bitagira umwandaElectrode

A107                                        

GB/T E308-15

AWS E308-15

Ibisobanuro: A107 ni electrode y'icyuma kitagira umukungugu ya Cr19Ni10 ifite karubone nkeya ifite sodium nkeya. Koresha DCEP (electrode y'amashanyarazi ifatika) kandi ishobora gusukurwa ahantu hose. Icyuma cyashyizwemo gifite imiterere myiza ya mekanike kandi kirwanya ingese hagati y'udusimba.

Ikoreshwa: Ikoreshwa mu gusudira inyubako z'icyuma kidashonga za 06Cr19Ni10 zirwanya ingese zifite ubushyuhe buri munsi ya 300°C. Ishobora kandi gusudira ibyuma bimwe na bimwe bidakoresha neza gusudira (nk'icyuma gifite chromium nyinshi) ndetse n'ibice by'icyuma kidashonga hejuru.

 

Imiterere ya shimi y'icyuma gisukwa (%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

18.0 ~ 21.0

9.0 ~ 11.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Imiterere ya tekiniki y'icyuma gisudira:

Ikintu cyo kugerageza

 

Imbaraga zo gukurura

Mpa

Kurekura

%

Yemejwe

≥550

≥35

 

Ikoreshwa ry'amashanyarazi risabwa:

Umwanya w'inkoni

(mm)

2.0

2.5

3.2

4.0

5.0

Umuyoboro wo gusudira

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Itangazo:

1. Electrode igomba gutekwa isaha imwe kuri 250℃ mbere yo gusudira;

2. Ubudahangarwa bw'ubushyuhe n'ingano ya ferrite mu byuma byabitswe bigenwa n'ubwumvikane bubiri bw'ibitangwa n'ibikenewe.

 

 

Wenzhou Tianyu Electronic Co., Ltd. yashinzwe mu 2000. Twakoze akazi ko gukora ibikoresho byaelectrode yo gusudiras, inkoni zo gusudira, naibikoresho byo gusudiraimyaka irenga 20.

Ibicuruzwa byacu by'ingenzi birimo icyuma kitagira umugeseelectrode yo gusudiras, electrode zo gusudira icyuma cya karuboni, electrode zo gusudira zifite alloy nkeya, electrode zo gusudira hejuru, electrode zo gusudira za nikeli na kobalti, insinga zo gusudira zifite icyuma gito n'alloy nkeya, insinga zo gusudira zifite icyuma kidafunze, insinga zikingira gazi, insinga zo gusudira za aluminiyumu, gusudira arc munsi y'amazi. insinga, insinga zo gusudira za nikeli na kobalti, insinga zo gusudira z'umuringa, insinga zo gusudira za TIG na MIG, electrode za tungsten, electrode zo gukata karuboni, n'ibindi bikoresho byo gusudira n'ibindi bikoresho byo gusudira.


  • Ibanjirije iyi:
  • Ibikurikira: