AWS A5.23: Insinga zo gusudira za ECF3 zicukuwe mu cyuma gikozwe mu cyuma gikozwe mu cyuma gito

Ibisobanuro bigufi:

AWS A5.23: Insinga za ECF3 zicukuwe mu cyuma gito cya Arc Cord, mu Bushinwa

Ibisobanuro birambuye ku gicuruzwa

Ibirango by'ibicuruzwa

ICYICIRO:

AWS A5.23: Insinga za ECF3 zicukuwe mu cyuma gikozwe mu cyuma gito gikozwe mu cyuma

IBISOBANURO:

AWS A5.23: ECF3 ni electrode y'insinga ifite insinga nkeya ikoreshwa mu gusudira arc munsi y'amazi mu buryo bukomeye. Kandi ihuye na chemistry ya AWS A5.23 F3, kandi yagenewe imbaraga zo gukurura zirenze 100 ksi.

IBIKORESHO N'INZUNGU:

Insinga zikozwe mu byuma zishobora gutanga igipimo cyiza cyo gushyiramo ugereranije n'insinga zikomeye kuri amperage zingana nazo.

Insinga zikozwe mu byuma zitanga uburyo bwagutse bwo kwinjira ugereranije n'insinga zikomeye ku bipimo byo gusudira bisa.

Ibisabwa ku miterere y'imiti yo gusukamo ubutare bisa n'iby'insinga zikomeye za EF3

Ibigize imiti ikoreshwa mu gusukamo ubutare bigizwe na nikeli iri munsi ya 1%

Ikomera cyane mu bushyuhe buke haba mu bihe byasutsweho ndetse no mu bihe bigabanya stress.

Bitanga amahirwe yo kongera umuvuduko w'ingendo kugira ngo umusaruro urusheho kwiyongera

Bifasha mu kwirinda gushya iyo usudira ku mugezi mwinshi ku mizi y'amazi n'ibikoresho bito cyane.

Ikwiriye nk'uburyo bwo kongera umusaruro mu bikorwa byinshi ubu ikoresha insinga ikomeye ya EF3

Ikwiriye gukoreshwa mu ikoreshwa rya gazi ihumanya aho ikibazo cy’ihungabana ry’ingufu ziterwa na hydrogen-sulfide ari ikibazo.

Bifasha kugabanya ibyago byo kwangirika mu bikorwa by'ingenzi no mu bikorwa bikomeye bya serivisi

INGANDA:

Gukora inyubako, peteroli na gaze, ikoreshwa ry'amashanyarazi, ibikoresho biremereye

UBWOKO BW'INSHINGANO:

Insinga y'icyuma-ifu, iy'icyuma-ifite insinga

UBU:

HN-590, SWX 120, SWX 150

IKIGANIRO:

Electrode y'Umuriro Igororotse (DCEP), Electrode y'Umuriro Igororotse (DCEN), Umuriro Uhindagurika (AC)

UBUBIKO:

Ibicuruzwa bigomba kubikwa ahantu humutse kandi hafungiye, kandi mu ipaki yabyo y'umwimerere imeze neza

INGINGO ZA AWS:

vava (4)

vava (3)

IMITUNGO ISANZWE YA KENIKI:

vava (5)

IBIPIMO BYA MBERE BY'IMIKORERE:

vava (1)

Gukomeza uburyo bwiza bwo gusudira - harimo no gushyushya mbere y'uko ibyuma bishyuha n'ubushyuhe bwo hagati y'ibyuma - bishobora kuba ingenzi bitewe n'ubwoko n'ubunini bw'icyuma gisudeshwa.

Ibipimo bitangwa ku mpamvu z'amakuru gusa. Agaciro kose ni akagereranyo. Voltage nziza ishobora gutandukana (ubusanzwe ni ± volts 2) bitewe n'amahitamo y'ihindagurika, ubunini bw'ibikoresho, imiterere y'ingingo, n'ibindi bintu byihariye bijyanye n'ikoreshwa.

Mu buryo nk'ubwo, igipimo nyacyo cyo gushyiramo ibintu gishobora gutandukana bitewe n'amahitamo y'uburyo ibintu bihinduka n'intera yo gukoraho.

UBURYO BWO GUPIKA:

vava (7)